Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.530 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.447 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP312 [149] |
HallP 3 2 |
Point Group32 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 294.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 158.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 80.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 300.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 135.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 282.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 339.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 158.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 333.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 271.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 233.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 33.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 233.6 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 166.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 300.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 22.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 166.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 249.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 248.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 158.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 166.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 57.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 161.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 322.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 113.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 271.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 333.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 300.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 300.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 203.9 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 201.7 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 310.4 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 322.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 300.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 90.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 66.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 161.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 100.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 161.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 231.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 66.7 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 166.9 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 300.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 294.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 203.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 271.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 271.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.01770 | 0.00000 | -0.00460 |
-0.00460 | 0.00460 | 0.00000 | 0.00000 | 0.01770 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.01885 C/m2 |
Crystallographic Direction vmax |
---|
-0.00000 |
1.00000 |
-0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.39 | 0.00 | 0.00 |
0.00 | 3.39 | 0.00 |
0.00 | 0.00 | 2.43 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.23 | 0.00 | 0.00 |
0.00 | 9.23 | 0.00 |
0.00 | 0.00 | 4.59 |
Polycrystalline dielectric constant
εpoly∞
3.07
|
Polycrystalline dielectric constant
εpoly
7.68
|
Refractive Index n1.75 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr(AsO3)2 (mp-983061) | 0.4797 | 0.000 | 3 |
Ba(SbO3)2 (mp-9127) | 0.4994 | 0.000 | 3 |
As2PbO6 (mp-20015) | 0.4241 | 0.000 | 3 |
TlSbO3 (mp-561465) | 0.5610 | 0.135 | 3 |
Sr(AsO3)2 (mp-754118) | 0.4601 | 0.000 | 3 |
RbPbIO6 (mp-616564) | 0.5740 | 0.000 | 4 |
RbSnIO6 (mp-554199) | 0.3855 | 0.000 | 4 |
KNiIO6 (mp-557733) | 0.2009 | 0.000 | 4 |
NaNiIO6 (mp-561926) | 0.6726 | 0.000 | 4 |
SrGeTeO6 (mp-10341) | 0.5985 | 0.000 | 4 |
BiI4 (mp-950217) | 0.5691 | 0.123 | 2 |
BiBr3 (mp-752602) | 0.6112 | 0.000 | 2 |
YBr3 (mp-754815) | 0.6146 | 0.000 | 2 |
BiBr3 (mp-568301) | 0.5745 | 0.002 | 2 |
CrCl3 (mp-569890) | 0.4275 | 0.001 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Ge_d I O |
Final Energy/Atom-5.1529 eV |
Corrected Energy-50.5896 eV
-50.5896 eV = -46.3759 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|