material

Ca(MnAs)2

ID:

mp-5498

DOI:

10.17188/1267397


Tags: Calcium dimanganese arsenide

Material Details

Final Magnetic Moment
5.222 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.471 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.079 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.13 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ca14MnAs11 + MnAs + Mn
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 41792 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.000 124.7
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.000 124.7
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.001 180.2
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.003 124.7
Mg (mp-153) <0 0 1> <0 0 1> 0.003 166.3
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.006 139.9
Mg (mp-153) <1 1 1> <1 1 0> 0.009 242.4
InAs (mp-20305) <1 1 1> <0 0 1> 0.012 263.3
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.012 221.7
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.017 263.3
PbSe (mp-2201) <1 0 0> <1 1 0> 0.021 193.9
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.021 166.3
WS2 (mp-224) <0 0 1> <0 0 1> 0.022 166.3
MgF2 (mp-1249) <1 0 0> <1 1 0> 0.023 145.4
GaSb (mp-1156) <1 0 0> <1 1 0> 0.025 193.9
TiO2 (mp-2657) <0 0 1> <1 1 0> 0.027 193.9
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.028 332.6
CdSe (mp-2691) <1 0 0> <1 1 0> 0.032 193.9
Mg (mp-153) <1 1 0> <0 0 1> 0.035 291.0
LaF3 (mp-905) <0 0 1> <0 0 1> 0.038 180.2
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.041 263.3
TePb (mp-19717) <1 1 1> <0 0 1> 0.044 221.7
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.051 124.7
GaN (mp-804) <1 1 1> <1 1 0> 0.052 242.4
NdGaO3 (mp-3196) <1 1 0> <1 1 0> 0.057 242.4
NaCl (mp-22862) <1 1 1> <0 0 1> 0.061 55.4
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.063 195.9
LiF (mp-1138) <1 1 1> <0 0 1> 0.068 263.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.073 180.2
GaSe (mp-1943) <0 0 1> <0 0 1> 0.073 166.3
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.075 221.7
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.075 110.9
SiC (mp-8062) <1 0 0> <1 1 0> 0.077 96.9
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.083 97.0
CdS (mp-672) <1 0 0> <1 1 0> 0.084 145.4
BN (mp-984) <1 0 1> <1 1 1> 0.089 100.8
SiC (mp-8062) <1 1 0> <1 1 1> 0.095 302.5
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.098 221.7
Ni (mp-23) <1 1 0> <0 0 1> 0.098 69.3
CdSe (mp-2691) <1 1 1> <0 0 1> 0.099 263.3
YAlO3 (mp-3792) <0 0 1> <1 0 1> 0.100 249.8
Si (mp-149) <1 0 0> <1 1 0> 0.100 242.4
CeO2 (mp-20194) <1 0 0> <1 1 0> 0.106 242.4
ZnTe (mp-2176) <1 0 0> <1 1 0> 0.109 193.9
Mg (mp-153) <1 0 1> <0 0 1> 0.110 207.9
Si (mp-149) <1 1 0> <1 0 1> 0.110 343.5
GaN (mp-804) <1 1 0> <0 0 1> 0.115 291.0
CeO2 (mp-20194) <1 1 0> <1 0 1> 0.117 343.5
Ni (mp-23) <1 0 0> <1 1 0> 0.121 48.5
InAs (mp-20305) <1 0 0> <1 1 0> 0.123 193.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
102 33 37 16 0 0
33 102 37 -16 0 0
37 37 121 0 0 0
16 -16 0 39 0 0
0 0 0 0 39 16
0 0 0 0 16 35
Compliance Tensor Sij (10-12Pa-1)
13.3 -4.4 -2.7 -7 0 0
-4.4 13.3 -2.7 7 0 0
-2.7 -2.7 9.9 0 0 0
-7 7 0 31 0 0
0 0 0 0 31 -14.1
0 0 0 0 -14.1 35.3
Shear Modulus GV
37 GPa
Bulk Modulus KV
60 GPa
Shear Modulus GR
31 GPa
Bulk Modulus KR
59 GPa
Shear Modulus GVRH
34 GPa
Bulk Modulus KVRH
60 GPa
Elastic Anisotropy
0.93
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Yb(MnAs)2 (mp-9592) 0.0560 0.040 3
Eu(MnAs)2 (mp-20128) 0.1004 0.059 3
Eu(MnSb)2 (mp-582227) 0.1946 0.211 3
Sr(AlGe)2 (mp-1070483) 0.1859 0.000 3
Sr(MnSb)2 (mp-2968) 0.0879 0.205 3
Li6Mn(FeO3)2 (mp-764386) 0.4808 0.040 4
LiFeCuS2 (mp-755288) 0.4009 0.124 4
Bi2O3 (mp-1017552) 0.4409 0.071 2
Pu2O3 (mp-21423) 0.5033 0.073 2
Mg3Bi2 (mp-569018) 0.5234 0.000 2
Ce2O3 (mp-2721) 0.5275 0.044 2
Mg3Sb2 (mp-2646) 0.4986 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Mn_pv As
Final Energy/Atom
-6.4008 eV
Corrected Energy
-32.0039 eV
-32.0039 eV = -32.0039 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 609906
  • 41792
Submitted by
User remarks:
  • Calcium dimanganese arsenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)