material

FeClO

ID:

mp-540828


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-1.651 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.31 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.914 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmmn [59]
Hall
P 2 2ab 1ab
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 16013 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 1 0> <1 0 0> 0.001 98.3
Au (mp-81) <1 1 0> <1 0 0> 0.002 98.3
Fe2O3 (mp-24972) <1 0 1> <1 1 0> 0.002 299.8
Fe2O3 (mp-24972) <1 0 0> <1 1 0> 0.003 214.1
Ga2O3 (mp-886) <1 1 0> <1 0 0> 0.004 294.9
WSe2 (mp-1821) <1 0 1> <1 1 0> 0.011 257.0
TiO2 (mp-2657) <1 0 1> <0 1 1> 0.012 152.4
GdScO3 (mp-5690) <0 1 1> <0 0 1> 0.012 272.5
AlN (mp-661) <0 0 1> <0 1 1> 0.012 152.4
MgF2 (mp-1249) <0 0 1> <0 1 0> 0.014 110.3
InAs (mp-20305) <1 1 0> <1 1 1> 0.015 268.5
CdS (mp-672) <1 0 0> <1 0 0> 0.015 229.3
Cu (mp-30) <1 1 0> <1 1 0> 0.017 128.5
Te2Mo (mp-602) <1 0 1> <1 0 1> 0.017 281.9
ZnTe (mp-2176) <1 1 0> <1 1 1> 0.019 268.5
MgF2 (mp-1249) <1 1 0> <0 1 1> 0.021 61.0
SrTiO3 (mp-4651) <1 1 1> <1 0 1> 0.021 70.5
Te2W (mp-22693) <0 0 1> <0 0 1> 0.022 155.7
LaAlO3 (mp-2920) <1 1 0> <0 1 1> 0.025 121.9
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.025 298.5
NaCl (mp-22862) <1 1 0> <0 1 1> 0.026 91.5
TiO2 (mp-2657) <1 1 1> <1 0 1> 0.027 176.2
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.029 129.8
Bi2Se3 (mp-541837) <1 0 0> <0 1 0> 0.031 248.2
TePb (mp-19717) <1 0 0> <0 0 1> 0.033 129.8
TePb (mp-19717) <1 1 0> <0 1 1> 0.033 61.0
Fe2O3 (mp-24972) <1 1 0> <1 0 1> 0.036 246.7
Ag (mp-124) <1 0 0> <0 1 0> 0.037 137.9
CdTe (mp-406) <1 1 0> <0 1 1> 0.037 61.0
TiO2 (mp-2657) <0 0 1> <0 1 0> 0.038 110.3
CaF2 (mp-2741) <1 1 1> <1 0 0> 0.038 262.1
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.039 155.7
TeO2 (mp-2125) <0 0 1> <0 1 0> 0.040 193.1
ZnSe (mp-1190) <1 1 0> <0 1 1> 0.040 91.5
Fe3O4 (mp-19306) <1 0 0> <1 1 0> 0.041 214.1
Cu (mp-30) <1 0 0> <1 1 0> 0.041 128.5
YVO4 (mp-19133) <0 0 1> <1 1 0> 0.042 257.0
InSb (mp-20012) <1 1 0> <0 1 1> 0.044 61.0
MgO (mp-1265) <1 0 0> <1 1 0> 0.044 128.5
CdS (mp-672) <1 0 1> <1 1 0> 0.047 128.5
YAlO3 (mp-3792) <0 1 1> <1 0 1> 0.049 141.0
CdS (mp-672) <1 1 0> <0 1 0> 0.049 248.2
TbScO3 (mp-31119) <0 1 1> <0 0 1> 0.050 272.5
Al2O3 (mp-1143) <1 1 0> <0 1 0> 0.050 110.3
WSe2 (mp-1821) <1 0 0> <0 1 1> 0.052 152.4
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.052 42.8
GaP (mp-2490) <1 1 0> <0 0 1> 0.053 129.8
GaP (mp-2490) <1 1 1> <1 0 0> 0.054 262.1
ZrO2 (mp-2858) <1 1 0> <0 1 0> 0.055 275.8
GaAs (mp-2534) <1 1 0> <0 1 1> 0.056 91.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.05 0.00 0.00
0.00 3.21 0.00
0.00 0.00 5.19
Dielectric Tensor εij (total)
9.34 0.00 0.00
0.00 3.79 0.00
0.00 0.00 15.72
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.15
Polycrystalline dielectric constant εpoly
(total)
9.62
Refractive Index n
2.04
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
InClO (mp-27702) 0.2590 0.000 3
AlClO (mp-27863) 0.1744 0.000 3
CrBrO (mp-31725) 0.2910 0.036 3
CrClO (mp-24905) 0.1523 0.000 3
VClO (mp-25118) 0.2664 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Fe_pv Cl O
Final Energy/Atom
-5.3961 eV
Corrected Energy
-78.9815 eV
Uncorrected energy = -64.7535 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Composition-based energy adjustment (-0.614 eV/atom x 4.0 atoms) = -2.4560 eV Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV Corrected energy = -78.9815 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 40963
  • 27136
  • 167393
  • 16013
Submitted by
User remarks:
  • Iron(III) oxide chloride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)