Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.977 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.52 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.467 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 413342 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-48) <0 0 1> <0 0 1> 0.000 163.5
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.001 303.7
CdTe (mp-406) <1 1 1> <0 0 1> 0.001 303.7
CdS (mp-672) <1 1 1> <1 0 1> 0.001 260.9
GaSe (mp-1943) <0 0 1> <0 0 1> 0.002 163.5
InSb (mp-20012) <1 1 1> <0 0 1> 0.002 303.7
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.002 93.5
LiTaO3 (mp-3666) <1 1 0> <1 1 0> 0.002 251.5
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.004 87.1
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.005 23.4
CdS (mp-672) <1 0 1> <1 0 0> 0.005 261.4
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.007 150.9
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.007 280.4
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.008 140.2
YAlO3 (mp-3792) <0 1 0> <1 0 0> 0.008 116.2
MgO (mp-1265) <1 1 1> <0 0 1> 0.009 93.5
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.013 210.3
GaN (mp-804) <1 1 0> <1 0 0> 0.016 29.0
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.016 210.3
KCl (mp-23193) <1 1 1> <0 0 1> 0.019 70.1
MgO (mp-1265) <1 1 0> <1 0 0> 0.019 232.4
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.020 23.4
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.021 116.8
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.021 319.5
WS2 (mp-224) <1 1 1> <1 0 0> 0.022 319.5
Ni (mp-23) <1 1 1> <0 0 1> 0.022 280.4
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.022 280.4
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.023 280.4
Mg (mp-153) <1 0 0> <1 0 0> 0.023 116.2
Fe2O3 (mp-24972) <1 1 1> <1 1 0> 0.024 251.5
GaN (mp-804) <0 0 1> <1 0 0> 0.025 145.2
CaF2 (mp-2741) <1 1 0> <1 0 0> 0.028 87.1
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 0 1> 0.028 149.1
SrTiO3 (mp-4651) <0 0 1> <1 1 0> 0.028 251.5
LiNbO3 (mp-3731) <1 0 0> <1 0 1> 0.029 74.5
Au (mp-81) <1 0 0> <1 0 1> 0.029 298.2
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.030 280.4
SiC (mp-7631) <0 0 1> <0 0 1> 0.030 210.3
GaN (mp-804) <1 0 0> <1 0 0> 0.031 116.2
BN (mp-984) <1 1 0> <1 0 1> 0.031 335.5
BN (mp-984) <0 0 1> <0 0 1> 0.031 70.1
SiO2 (mp-6930) <1 1 0> <1 0 0> 0.033 145.2
LiNbO3 (mp-3731) <1 1 0> <1 1 0> 0.033 251.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.033 210.3
InP (mp-20351) <1 1 0> <1 0 1> 0.034 149.1
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.035 261.4
AlN (mp-661) <0 0 1> <0 0 1> 0.037 163.5
ZnO (mp-2133) <1 0 1> <1 1 1> 0.038 277.3
GaP (mp-2490) <1 1 0> <1 0 0> 0.039 87.1
SiC (mp-8062) <1 1 1> <0 0 1> 0.039 303.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
34 14 9 2 0 0
14 34 9 -2 0 0
9 9 24 0 0 0
2 -2 0 5 0 0
0 0 0 0 5 2
0 0 0 0 2 10
Compliance Tensor Sij (10-12Pa-1)
38.6 -14.1 -9 -17.5 0 0
-14.1 38.6 -9 17.5 0 0
-9 -9 48 0 0 0
-17.5 17.5 0 214.6 0 0
0 0 0 0 214.6 -35.1
0 0 0 0 -35.1 105.4
Shear Modulus GV
8 GPa
Bulk Modulus KV
17 GPa
Shear Modulus GR
7 GPa
Bulk Modulus KR
16 GPa
Shear Modulus GVRH
7 GPa
Bulk Modulus KVRH
17 GPa
Elastic Anisotropy
0.99
Poisson's Ratio
0.31

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.36 -0.00 0.00
-0.00 5.36 -0.00
0.00 -0.00 3.04
Dielectric Tensor εij (total)
11.22 -0.00 0.00
-0.00 11.22 -0.00
0.00 -0.00 5.28
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.58
Polycrystalline dielectric constant εpoly
(total)
9.24
Refractive Index n
2.14
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CsAu3Se2 (mp-9386) 0.5300 0.000 3
RbAu3Se2 (mp-9385) 0.6150 0.000 3
CsAu3S2 (mp-9384) 0.5105 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cs_sv Cu_pv O
Final Energy/Atom
-4.5907 eV
Corrected Energy
-28.9485 eV
-28.9485 eV = -27.5439 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 413342
Submitted by
User remarks:
  • Cesium dioxotricuprate(I)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)