material

TiO2

ID:

mp-553432

DOI:

10.17188/1267616


Tags: Titanium oxide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.453 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.049 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.38 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
TiO2
Band Gap
3.421 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3121 [152]
Hall
P 31 2"
Point Group
32
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <1 1 0> <1 1 1> 0.000 262.2
TeO2 (mp-2125) <0 1 0> <1 0 0> 0.003 68.8
BN (mp-984) <1 1 1> <1 0 1> 0.004 307.5
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.004 327.8
AlN (mp-661) <0 0 1> <0 0 1> 0.010 109.3
C (mp-66) <1 0 0> <1 0 0> 0.011 240.9
LiAlO2 (mp-3427) <1 0 1> <1 1 0> 0.012 298.0
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.012 191.2
Mg (mp-153) <1 0 0> <1 0 1> 0.016 219.7
GaN (mp-804) <1 1 0> <1 0 1> 0.017 87.9
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.017 327.8
TeO2 (mp-2125) <1 0 1> <1 0 1> 0.018 307.5
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.018 172.0
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.018 218.5
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.019 172.0
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.019 178.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.023 109.3
Ag (mp-124) <1 1 1> <0 0 1> 0.023 355.1
C (mp-48) <0 0 1> <0 0 1> 0.024 109.3
SiC (mp-11714) <0 0 1> <0 0 1> 0.025 109.3
Bi2Te3 (mp-34202) <0 0 1> <1 0 1> 0.027 307.5
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.029 54.6
SrTiO3 (mp-4651) <1 0 0> <1 1 1> 0.035 131.1
GaTe (mp-542812) <1 0 0> <1 0 0> 0.035 309.7
GaN (mp-804) <0 0 1> <0 0 1> 0.035 27.3
CdS (mp-672) <1 1 0> <1 1 1> 0.035 196.7
CsI (mp-614603) <1 1 0> <1 1 1> 0.038 262.2
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.038 275.3
LiGaO2 (mp-5854) <1 1 1> <1 0 0> 0.039 275.3
C (mp-48) <1 0 1> <1 0 1> 0.039 263.6
BN (mp-984) <0 0 1> <0 0 1> 0.040 327.8
ZnO (mp-2133) <1 0 0> <1 1 1> 0.044 262.2
Te2W (mp-22693) <0 0 1> <1 0 0> 0.044 309.7
CdS (mp-672) <0 0 1> <0 0 1> 0.045 109.3
KCl (mp-23193) <1 1 0> <1 0 1> 0.045 175.7
Au (mp-81) <1 1 1> <0 0 1> 0.046 355.1
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.050 163.9
GaTe (mp-542812) <1 0 -1> <1 0 0> 0.053 309.7
C (mp-48) <1 0 0> <1 1 1> 0.053 196.7
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.053 172.0
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.056 172.0
CdS (mp-672) <1 0 0> <1 0 0> 0.057 309.7
Cu (mp-30) <1 1 1> <0 0 1> 0.058 355.1
PbS (mp-21276) <1 1 1> <0 0 1> 0.058 191.2
CsI (mp-614603) <1 1 1> <0 0 1> 0.059 109.3
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.060 163.9
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.063 240.9
MoS2 (mp-1434) <1 1 1> <1 0 0> 0.065 240.9
TiO2 (mp-390) <1 0 0> <0 0 1> 0.066 109.3
MgO (mp-1265) <1 1 0> <1 0 0> 0.066 103.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
42 5 3 3 0 0
5 42 3 -3 0 0
3 3 26 0 0 0
3 -3 0 11 0 0
0 0 0 0 11 3
0 0 0 0 3 18
Compliance Tensor Sij (10-12Pa-1)
24.9 -3.2 -2.3 -7.5 0 0
-3.2 24.9 -2.3 7.5 0 0
-2.3 -2.3 39.3 0 0 0
-7.5 7.5 0 98.7 0 0
0 0 0 0 98.7 -15
0 0 0 0 -15 56.3
Shear Modulus GV
15 GPa
Bulk Modulus KV
14 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
14 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
14 GPa
Elastic Anisotropy
0.63
Poisson's Ratio
0.13

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.05731 -0.05731 0.00000 0.05543 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 -0.05543 -0.05731
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.09819 C/m2
Crystallographic Direction vmax
-1.00000
0.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.77 0.00 0.00
0.00 3.77 0.00
0.00 0.00 3.92
Dielectric Tensor εij (total)
8.44 0.00 -0.00
0.00 8.44 0.00
-0.00 0.00 9.24
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.82
Polycrystalline dielectric constant εpoly
(total)
8.70
Refractive Index n
1.95
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AlPO4 (mp-7848) 0.2610 0.000 3
AlPO4 (mp-3955) 0.2414 0.009 3
AlPO4 (mp-4051) 0.2740 0.002 3
BePO4 (mp-760410) 0.1914 0.064 3
AlPO4 (mp-5331) 0.2417 0.009 3
CsBeAsO4 (mp-9113) 0.6921 0.000 4
Cs2MgSi5O12 (mp-1019610) 0.7009 0.000 4
WN2 (mp-754629) 0.1861 0.102 2
SiO2 (mp-7000) 0.1079 0.011 2
SiO2 (mp-12787) 0.1590 0.010 2
BeF2 (mp-15951) 0.0393 0.000 2
SiO2 (mp-6930) 0.1011 0.010 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Mesoporous TiO2 photocatalysts have been synthesized using polyethylene glycol (PEG) as a template direction agent in diluted acetic acid aqueous solution. This medium slows down the hydrolysis reacti [...]
Aluminum pillared clay (Al-PILC) and platinum impregnated pillared clay (Pt/Al-PILC) were prepared, characterized and tested as catalysts in adipic ester hydrogenation. Results were compared with thos [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition TiO2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv O
Final Energy/Atom
-8.9250 eV
Corrected Energy
-84.4469 eV
Uncorrected energy = -80.3249 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Corrected energy = -84.4469 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 41493
Submitted by
User remarks:
  • Titanium oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)