Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.357 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.026 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn3(PO4)2 |
Band Gap3.334 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 275.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 246.3 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 246.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 275.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 164.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 206.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 246.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 275.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 82.1 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 176.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 265.1 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 275.5 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 164.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 82.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 208.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 233.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 82.1 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 88.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 246.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 164.2 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 246.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 133.4 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 -1> | 265.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 82.1 |
Al (mp-134) | <1 1 0> | <0 1 1> | 208.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 233.7 |
CdTe (mp-406) | <1 0 0> | <1 0 -1> | 88.4 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 246.3 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 208.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 233.7 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 246.3 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 246.3 |
TiO2 (mp-2657) | <0 0 1> | <1 0 -1> | 88.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 82.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 275.5 |
C (mp-66) | <1 1 0> | <1 0 0> | 164.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 164.2 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 206.7 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 155.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 155.8 |
InSb (mp-20012) | <1 0 0> | <1 0 -1> | 88.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 246.3 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 275.5 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 164.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 233.7 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 233.7 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 -1> | 265.1 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 -1> | 265.1 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 233.7 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 164.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu4(PO4)3 (mp-673151) | 0.5022 | 0.039 | 3 |
Mg3(AsO4)2 (mp-770734) | 0.4952 | 0.065 | 3 |
Mn3(PO4)2 (mp-770563) | 0.4770 | 0.015 | 3 |
Fe3(PO4)2 (mp-636647) | 0.4218 | 0.000 | 3 |
Ni3(PO4)2 (mp-771911) | 0.4316 | 0.192 | 3 |
LiCuPO4 (mp-758497) | 0.4890 | 0.081 | 4 |
LiCu4(PO4)3 (mp-673145) | 0.4984 | 0.062 | 4 |
NaCoPO4 (mp-683773) | 0.5018 | 0.038 | 4 |
LiFe4(PO4)3 (mp-762839) | 0.4811 | 0.285 | 4 |
NaMg4(PO4)3 (mp-560981) | 0.4929 | 0.028 | 4 |
LiMn2P2HO8 (mp-767685) | 0.7010 | 0.037 | 5 |
LiFe2P2HO8 (mp-763773) | 0.7083 | 0.024 | 5 |
Na2LiVPO6 (mp-763825) | 0.6924 | 0.094 | 5 |
Na2Li2V3P2O13 (mp-853239) | 0.6670 | 0.061 | 5 |
K2Mn2Zn4Si4O15 (mp-567173) | 0.6491 | 0.004 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn P O |
Final Energy/Atom-6.0930 eV |
Corrected Energy-339.3090 eV
-339.3090 eV = -316.8357 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)