Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.956 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa2Ni7F18 + BaF2 |
Band Gap4.830 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 287.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 335.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 143.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 239.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 335.4 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 210.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 191.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 113.1 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 105.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 335.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 210.5 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 210.5 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 143.7 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 105.2 |
InP (mp-20351) | <1 0 0> | <1 0 -1> | 105.2 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 191.7 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 105.2 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 335.4 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 239.6 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 -1> | 210.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 1 -1> | 173.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 191.7 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 335.4 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 239.6 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 143.7 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 143.7 |
Si (mp-149) | <1 0 0> | <1 0 0> | 239.6 |
Au (mp-81) | <1 0 0> | <1 0 -1> | 105.2 |
Au (mp-81) | <1 1 1> | <1 0 0> | 239.6 |
C (mp-48) | <0 0 1> | <1 0 0> | 287.5 |
C (mp-48) | <1 0 0> | <1 0 0> | 95.8 |
C (mp-48) | <1 1 0> | <1 0 0> | 239.6 |
NaCl (mp-22862) | <1 1 1> | <1 0 0> | 335.4 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 287.5 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 239.6 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 335.4 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 239.6 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 -1> | 210.5 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 95.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 226.3 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 191.7 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 287.5 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 143.7 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 239.6 |
ZnO (mp-2133) | <0 0 1> | <1 0 0> | 239.6 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 138.5 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 191.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 239.6 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 105.2 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 239.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: F Ni_pv Ba_sv |
Final Energy/Atom-4.8827 eV |
Corrected Energy-159.4661 eV
-159.4661 eV = -146.4821 eV (uncorrected energy) - 12.9840 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)