Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.886 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.245 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCF4 + TeF4 + C |
Band Gap4.404 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 275.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 275.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 275.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 275.0 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 183.3 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 275.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 275.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 183.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 275.0 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 275.0 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 275.0 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 183.3 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 91.7 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 275.0 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 183.3 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 275.0 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 183.3 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 0> | 275.0 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 0> | 275.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SiH3I (mp-28538) | 0.5977 | 0.000 | 3 |
Zn(HO)2 (mp-625826) | 0.6693 | 0.082 | 3 |
Pd(SCl3)2 (mp-28174) | 0.5977 | 0.000 | 3 |
GeH3Cl (mp-28369) | 0.5915 | 0.000 | 3 |
Si3PH9 (mp-28842) | 0.6635 | 0.000 | 3 |
P2H9(CBr)3 (mp-779221) | 0.5800 | 0.000 | 4 |
H9PbC3I (mp-760193) | 0.6547 | 0.206 | 4 |
LiCu(HO)4 (mp-759472) | 0.6106 | 0.082 | 4 |
BPH9C2 (mp-758984) | 0.6444 | 0.072 | 4 |
CIClF4 (mp-556844) | 0.4633 | 0.205 | 4 |
PH9C3Br3N (mp-24283) | 0.6395 | 0.135 | 5 |
InSi2As(H3C)8 (mp-568872) | 0.6038 | 0.073 | 5 |
H3CSClO (mp-644221) | 0.6388 | 0.245 | 5 |
ZnSi4As2(H3C)12 (mp-570146) | 0.5547 | 0.044 | 5 |
InSi2P(H3C)8 (mp-569070) | 0.6328 | 0.066 | 5 |
H3CSN(ClO)2 (mp-558736) | 0.6409 | 0.455 | 6 |
NaH12C4S2BrO2 (mp-555975) | 0.6276 | 0.138 | 6 |
CdSi3PH27C9Br2 (mp-604998) | 0.7161 | 0.018 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te C F |
Final Energy/Atom-4.8817 eV |
Corrected Energy-322.1906 eV
-322.1906 eV = -322.1906 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)