Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-1.935 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.656 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63 [173] |
HallP 6c |
Point Group6 |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 264.8 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 100.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 264.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 290.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 211.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 232.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 116.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 58.1 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 58.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 264.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 174.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 232.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 232.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 116.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.3 |
GaSe (mp-1943) | <1 0 1> | <1 1 0> | 201.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 174.3 |
BN (mp-984) | <1 1 0> | <1 1 1> | 133.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 290.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 232.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 264.8 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 100.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 290.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 100.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 116.2 |
Al (mp-134) | <1 0 0> | <1 0 0> | 290.5 |
Al (mp-134) | <1 1 1> | <1 0 0> | 58.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 264.8 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 232.4 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 232.4 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 232.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 264.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 290.5 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 58.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.3 |
GaSe (mp-1943) | <1 0 0> | <1 1 0> | 201.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 116.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 174.3 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 290.5 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 290.5 |
C (mp-66) | <1 1 0> | <1 0 0> | 232.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 88.3 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 290.5 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 232.4 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 0> | 174.3 |
MoSe2 (mp-1634) | <1 1 1> | <1 0 0> | 174.3 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 232.4 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 290.5 |
GdScO3 (mp-5690) | <1 1 0> | <1 1 0> | 201.3 |
Au (mp-81) | <1 0 0> | <1 0 0> | 174.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd3SiCuSe7 (mp-641534) | 0.1014 | 0.000 | 4 |
Pr3SiCuSe7 (mp-568801) | 0.0993 | 0.000 | 4 |
Nd3SiCuS7 (mp-556975) | 0.0679 | 0.000 | 4 |
La3SiCuSe7 (mp-568082) | 0.0771 | 0.000 | 4 |
Tb3SiCuS7 (mp-560501) | 0.1144 | 0.000 | 4 |
GaBr2 (mp-650841) | 0.6203 | 0.010 | 2 |
Rb2WO4 (mp-18864) | 0.6561 | 0.000 | 3 |
U3Cu2Se7 (mp-541587) | 0.4607 | 0.000 | 3 |
U3Cu2S7 (mp-619067) | 0.4276 | 0.000 | 3 |
Rb2MoO4 (mp-19212) | 0.6531 | 0.000 | 3 |
Cs2WO4 (mp-761354) | 0.6580 | 0.000 | 3 |
KBiS(ClO2)2 (mp-23645) | 0.7353 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points20 |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Cu_pv Si Cu_pv S |
Final Energy/Atom-5.9289 eV |
Corrected Energy-151.5819 eV
-151.5819 eV = -142.2935 eV (uncorrected energy) - 9.2884 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)