Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.273 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.715 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4 [82] |
HallI 4 |
Point Group4 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-66) | <1 0 0> | <1 0 0> | 308.5 |
C (mp-66) | <1 1 0> | <1 0 0> | 88.1 |
C (mp-66) | <1 1 1> | <1 0 0> | 44.1 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 311.6 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 176.3 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 308.9 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 249.3 |
Mg (mp-153) | <1 0 1> | <1 1 1> | 297.7 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 220.3 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 231.7 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 264.4 |
LaF3 (mp-905) | <1 0 1> | <1 0 1> | 266.8 |
LaF3 (mp-905) | <1 1 0> | <1 1 0> | 187.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 220.3 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 264.4 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 154.5 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 308.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 308.9 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 311.6 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 311.6 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 308.9 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 220.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 88.1 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 44.1 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 77.2 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 220.3 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 132.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 249.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 308.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 1 1> | 198.5 |
NdGaO3 (mp-3196) | <0 1 1> | <1 1 0> | 311.6 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 308.9 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 352.6 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 352.6 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 264.4 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 132.2 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 308.5 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 0> | 187.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 1 0> | 187.0 |
Si (mp-149) | <1 0 0> | <0 0 1> | 154.5 |
Si (mp-149) | <1 1 1> | <1 0 0> | 308.5 |
Au (mp-81) | <1 0 0> | <0 0 1> | 154.5 |
Au (mp-81) | <1 1 0> | <1 0 0> | 352.6 |
Au (mp-81) | <1 1 1> | <1 0 0> | 88.1 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 77.2 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 220.3 |
CdSe (mp-2691) | <1 1 1> | <1 0 0> | 132.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 231.7 |
C (mp-48) | <1 0 0> | <1 1 0> | 249.3 |
C (mp-48) | <1 0 1> | <1 1 0> | 311.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.03784 | -0.03784 | 0.02604 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.00686 | 0.13981 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.13981 | -0.00686 |
Piezoelectric Modulus ‖eij‖max0.13998 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-0.00000 |
-1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.15 | 0.00 | 0.00 |
0.00 | 2.15 | 0.00 |
0.00 | 0.00 | 2.15 |
Dielectric Tensor εij (total) |
||
---|---|---|
3.68 | -0.00 | 0.00 |
-0.00 | 3.76 | 0.00 |
0.00 | 0.00 | 3.76 |
Polycrystalline dielectric constant
εpoly∞
2.15
|
Polycrystalline dielectric constant
εpoly
3.73
|
Refractive Index n1.47 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-7848) | 0.3013 | 0.000 | 3 |
AlPO4 (mp-3955) | 0.3093 | 0.009 | 3 |
BePO4 (mp-760410) | 0.1903 | 0.063 | 3 |
AlPO4 (mp-555941) | 0.3163 | 0.011 | 3 |
AlPO4 (mp-5331) | 0.3095 | 0.009 | 3 |
CsBeAsO4 (mp-9113) | 0.7287 | 0.000 | 4 |
Cs2MgSi5O12 (mp-1019610) | 0.6937 | 0.000 | 4 |
SiO2 (mp-559550) | 0.1455 | 0.008 | 2 |
SiO2 (mp-554089) | 0.1391 | 0.003 | 2 |
SiO2 (mp-7000) | 0.1745 | 0.011 | 2 |
SiO2 (mp-600028) | 0.1665 | 0.013 | 2 |
SiO2 (mp-12787) | 0.1442 | 0.010 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9112 eV |
Corrected Energy-100.5522 eV
-100.5522 eV = -94.9339 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)