material

Tl2Ni3S2

ID:

mp-554212

DOI:

10.17188/1267798


Tags: Nickel thallium suldide (3/2/2) Dithallium trinickel disulfide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.466 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.003 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.73 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ni3S2 + Tl2S + Ni
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WS2 (mp-224) <0 0 1> <0 0 1> 0.004 26.5
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.004 26.5
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.004 106.1
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.005 77.3
Mg (mp-153) <1 1 0> <1 0 0> 0.006 231.8
GaSe (mp-1943) <0 0 1> <0 0 1> 0.007 238.8
LiF (mp-1138) <1 1 1> <0 0 1> 0.008 345.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.009 79.6
CsI (mp-614603) <1 0 0> <1 0 0> 0.011 309.1
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.011 159.2
GdScO3 (mp-5690) <0 1 1> <1 0 1> 0.012 163.4
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.014 309.1
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.014 154.6
AlN (mp-661) <0 0 1> <0 0 1> 0.015 238.8
Ni (mp-23) <1 0 0> <1 0 0> 0.016 309.1
Te2W (mp-22693) <0 1 1> <1 0 0> 0.016 231.8
InP (mp-20351) <1 1 1> <0 0 1> 0.021 185.7
Mg (mp-153) <0 0 1> <0 0 1> 0.022 26.5
GaN (mp-804) <1 1 0> <1 0 0> 0.022 231.8
CsI (mp-614603) <1 1 1> <0 0 1> 0.024 106.1
PbS (mp-21276) <1 1 1> <0 0 1> 0.026 185.7
WS2 (mp-224) <1 1 1> <0 0 1> 0.026 79.6
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.031 309.1
CdS (mp-672) <0 0 1> <0 0 1> 0.044 106.1
Si (mp-149) <1 1 0> <0 0 1> 0.046 212.3
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.047 309.1
Al (mp-134) <1 0 0> <0 0 1> 0.047 291.9
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.047 185.7
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.048 212.3
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.050 159.2
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.050 53.1
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.052 309.1
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.053 106.1
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.054 154.6
GaN (mp-804) <1 1 1> <1 0 0> 0.057 154.6
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.057 185.7
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.060 159.2
GaTe (mp-542812) <1 0 0> <0 0 1> 0.061 318.4
GaN (mp-804) <0 0 1> <0 0 1> 0.063 26.5
LiGaO2 (mp-5854) <0 0 1> <1 0 0> 0.064 309.1
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.071 53.1
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.073 309.1
Ni (mp-23) <1 1 0> <0 0 1> 0.076 345.0
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.083 53.1
GaP (mp-2490) <1 1 0> <0 0 1> 0.083 212.3
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.084 309.1
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.084 154.6
SiC (mp-11714) <0 0 1> <0 0 1> 0.091 106.1
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.094 238.8
BN (mp-984) <0 0 1> <0 0 1> 0.095 238.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
88 52 33 -5 -0 0
52 88 33 5 -0 0
33 33 78 0 -0 0
-5 5 0 25 0 -0
-0 -0 -0 0 25 -5
0 -0 0 -0 -5 18
Compliance Tensor Sij (10-12Pa-1)
19 -10 -3.8 5.8 0 0
-10 19 -3.8 -5.8 0 0
-3.8 -3.8 16 0 0 0
5.8 -5.8 0 42.7 0 0
0 0 0 0 42.7 11.7
0 0 0 0 11.7 58
Shear Modulus GV
23 GPa
Bulk Modulus KV
54 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
53 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
54 GPa
Elastic Anisotropy
0.44
Poisson's Ratio
0.32

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
28
U Values
--
Pseudopotentials
VASP PAW: Tl_d Ni_pv S
Final Energy/Atom
-4.6084 eV
Corrected Energy
-33.5861 eV
-33.5861 eV = -32.2591 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 422328
  • 108893

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)