material

TiO2

ID:

mp-554278

DOI:

10.17188/1267830


Tags: Titanium oxide - beta Titanium oxide - (B)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.512 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.62 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.694 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/m [12]
Hall
-C 2y
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 41056 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <1 0 1> <1 0 0> 0.009 324.0
AlN (mp-661) <1 0 0> <1 0 1> 0.013 234.7
InSb (mp-20012) <1 1 0> <1 0 0> 0.016 124.6
CdTe (mp-406) <1 1 0> <1 0 0> 0.020 124.6
TiO2 (mp-390) <1 1 1> <1 1 -1> 0.023 271.1
NdGaO3 (mp-3196) <1 0 0> <1 0 1> 0.036 176.1
C (mp-66) <1 0 0> <1 1 1> 0.037 292.6
LiGaO2 (mp-5854) <1 1 1> <1 0 0> 0.042 224.3
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.045 163.6
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.048 174.5
CdTe (mp-406) <1 0 0> <1 0 0> 0.051 174.5
SiC (mp-7631) <1 0 0> <1 0 1> 0.059 234.7
CdS (mp-672) <0 0 1> <1 0 0> 0.064 199.4
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.066 174.5
InSb (mp-20012) <1 0 0> <1 0 0> 0.068 174.5
ZnTe (mp-2176) <1 1 1> <1 0 0> 0.068 199.4
MoS2 (mp-1434) <1 0 1> <0 1 1> 0.070 271.9
InAs (mp-20305) <1 1 1> <1 0 0> 0.073 199.4
ZnO (mp-2133) <0 0 1> <1 0 0> 0.073 74.8
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.073 174.5
CdS (mp-672) <1 0 1> <1 0 0> 0.074 324.0
TiO2 (mp-2657) <1 0 0> <1 1 1> 0.076 97.5
LiF (mp-1138) <1 1 1> <1 0 0> 0.091 174.5
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.091 174.5
Te2W (mp-22693) <1 0 0> <1 0 1> 0.098 293.4
BN (mp-984) <1 0 1> <0 1 1> 0.098 181.3
CdSe (mp-2691) <1 1 1> <1 0 0> 0.100 199.4
YAlO3 (mp-3792) <0 1 0> <1 0 1> 0.100 117.4
TePb (mp-19717) <1 0 0> <1 0 0> 0.103 174.5
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.104 199.4
MgF2 (mp-1249) <1 0 1> <1 0 -1> 0.110 183.2
TeO2 (mp-2125) <0 1 0> <1 0 -1> 0.113 137.4
GaSb (mp-1156) <1 1 1> <1 0 0> 0.125 199.4
CaCO3 (mp-3953) <1 0 0> <1 0 0> 0.127 174.5
Ni (mp-23) <1 1 0> <1 0 0> 0.132 174.5
BN (mp-984) <1 0 0> <1 0 0> 0.135 174.5
CdS (mp-672) <1 0 0> <1 0 -1> 0.159 320.5
BN (mp-984) <1 1 0> <1 0 0> 0.159 99.7
PbSe (mp-2201) <1 1 1> <1 0 0> 0.165 199.4
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 0 0> 0.165 199.4
ZnSe (mp-1190) <1 1 0> <1 0 0> 0.173 324.0
C (mp-48) <0 0 1> <1 0 0> 0.176 74.8
BN (mp-984) <0 0 1> <1 0 0> 0.178 49.8
GaSe (mp-1943) <1 0 1> <1 0 -1> 0.181 137.4
LiAlO2 (mp-3427) <1 0 0> <1 0 1> 0.184 293.4
SiO2 (mp-6930) <1 1 1> <1 0 -1> 0.197 320.5
NaCl (mp-22862) <1 1 0> <1 0 0> 0.203 324.0
ZrO2 (mp-2858) <1 0 0> <0 1 0> 0.205 311.6
GaSe (mp-1943) <0 0 1> <1 0 0> 0.211 24.9
GaAs (mp-2534) <1 1 0> <1 0 0> 0.212 324.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
270 139 135 0 -10 0
139 311 117 0 -15 0
135 117 270 0 12 0
0 0 0 58 0 -4
-10 -15 12 0 57 0
0 0 0 -4 0 46
Compliance Tensor Sij (10-12Pa-1)
5.7 -1.7 -2.1 0 1 0
-1.7 4.4 -1.1 0 1.1 0
-2.1 -1.1 5.3 0 -1.8 0
0 0 0 17.3 0 1.7
1 1.1 -1.8 0 18.4 0
0 0 0 1.7 0 22.1
Shear Modulus GV
63 GPa
Bulk Modulus KV
181 GPa
Shear Modulus GR
59 GPa
Bulk Modulus KR
180 GPa
Shear Modulus GVRH
61 GPa
Bulk Modulus KVRH
181 GPa
Elastic Anisotropy
0.35
Poisson's Ratio
0.35

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
6.12 0.00 0.15
0.00 6.28 0.00
0.15 0.00 6.21
Dielectric Tensor εij (total)
31.30 0.00 1.83
0.00 38.90 0.00
1.83 0.00 36.22
Polycrystalline dielectric constant εpoly
(electronic contribution)
6.21
Polycrystalline dielectric constant εpoly
(total)
35.47
Refractive Index n
2.49
Potentially ferroelectric?
Unknown

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -8.974 12.249 10.823 5.684
pack_evans_james -8.974 12.250 1.199 3.231
vinet -8.975 12.243 10.995 4.938
tait -8.975 12.241 1.214 5.364
birch_euler -8.974 12.248 1.356 0.237
pourier_tarantola -8.976 12.240 0.207 2.284
birch_lagrange -8.984 12.245 0.767 5.975
murnaghan -8.972 12.262 1.173 3.105
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NbGaO4 (mp-7601) 0.4214 0.000 3
V3FeO8 (mp-766844) 0.4221 0.306 3
MnV3O8 (mp-776217) 0.4002 0.057 3
V3FeO8 (mp-771199) 0.3971 0.043 3
TiV3O8 (mp-849354) 0.2976 0.029 3
Li2VOF4 (mp-780857) 0.6472 0.000 4
Li2VOF4 (mp-764695) 0.6953 0.009 4
Li2V4O5F8 (mp-764711) 0.4766 0.079 4
AlNi(WO4)2 (mvc-613) 0.7272 0.231 4
V6O13 (mp-714921) 0.4749 0.064 2
ZrO2 (mp-755769) 0.1515 0.052 2
NbO2 (mp-754698) 0.2149 0.107 2
VO2 (mp-561637) 0.4033 0.030 2
V6O13 (mp-18896) 0.4539 0.023 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Mesoporous TiO2 photocatalysts have been synthesized using polyethylene glycol (PEG) as a template direction agent in diluted acetic acid aqueous solution. This medium slows down the hydrolysis reacti [...]
Aluminum pillared clay (Al-PILC) and platinum impregnated pillared clay (Pt/Al-PILC) were prepared, characterized and tested as catalysts in adipic ester hydrogenation. Results were compared with thos [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition TiO2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv O
Final Energy/Atom
-8.9741 eV
Corrected Energy
-113.1851 eV
Uncorrected energy = -107.6891 eV Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV Corrected energy = -113.1851 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 41056
  • 57449
  • 171670
  • 57154
Submitted by
User remarks:
  • Titanium oxide - (B)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)