Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.433 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.947 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP31m [157] |
HallP 3 2 |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 131.6 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 263.2 |
Au (mp-81) | <1 0 0> | <0 0 1> | 263.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 131.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 131.6 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 131.6 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 174.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3SiO5 (mp-558273) | 0.4524 | 0.050 | 3 |
Ba3GeO5 (mp-770959) | 0.5162 | 0.019 | 3 |
Ba3GeO5 (mp-756637) | 0.5024 | 0.027 | 3 |
Ca3SiO5 (mp-641754) | 0.5131 | 0.020 | 3 |
Ca3SiO5 (mp-27917) | 0.5465 | 0.062 | 3 |
Li2CrPO5 (mp-761451) | 0.6665 | 0.146 | 4 |
Na3SO4F (mp-560222) | 0.3920 | 0.000 | 4 |
Na3WO4F (mp-565594) | 0.6078 | 0.004 | 4 |
LiCdPO4 (mp-556786) | 0.6588 | 0.000 | 4 |
CrAg3ClO4 (mp-566124) | 0.6478 | 0.022 | 4 |
Na2CaPO4F (mp-39260) | 0.4078 | 0.027 | 5 |
Na2MnPO4F (mp-566286) | 0.5060 | 0.595 | 5 |
Na2CoPO4F (mp-19563) | 0.5203 | 0.113 | 5 |
Na21S7Cl(O14F3)2 (mp-680169) | 0.1545 | 0.002 | 5 |
Li2VPO4F (mp-849509) | 0.5403 | 0.365 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv S Cl O F |
Final Energy/Atom-5.2972 eV |
Corrected Energy-769.4331 eV
Uncorrected energy = -715.1241 eV
Composition-based energy adjustment (-0.503 eV/atom x 15.0 atoms) = -7.5450 eV
Composition-based energy adjustment (-0.687 eV/atom x 60.0 atoms) = -41.2200 eV
Composition-based energy adjustment (-0.462 eV/atom x 12.0 atoms) = -5.5440 eV
Corrected energy = -769.4331 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)