Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.876 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGaN + ZnO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 109.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 328.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 36.5 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 124.0 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 124.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 182.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 255.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 255.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 182.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 68.4 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 77.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 118.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 146.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 310.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 205.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 182.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 255.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 292.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 182.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 182.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 182.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 255.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 109.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 109.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 68.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 255.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 182.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 109.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 219.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 255.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 328.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 182.6 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 205.3 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 205.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 136.9 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 310.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 328.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 146.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 273.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 219.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 292.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 109.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 328.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 255.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 109.6 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 219.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 255.7 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 232.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 273.8 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 109.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgGeN2 (mp-7798) | 0.3055 | 0.000 | 3 |
Li3CuF4 (mp-752895) | 0.2475 | 0.097 | 3 |
Li3VS4 (mp-755642) | 0.3043 | 0.036 | 3 |
LiGe2N3 (mp-1020059) | 0.2279 | 0.000 | 3 |
Li2SnSe3 (mp-1095291) | 0.3122 | 0.000 | 3 |
Cu2HgGeS4 (mp-557574) | 0.2202 | 0.002 | 4 |
ZnGa3N3O (mp-554674) | 0.1403 | 0.048 | 4 |
ZnGaNO (mp-558498) | 0.1549 | 0.075 | 4 |
ZnGaNO (mp-560887) | 0.0966 | 0.073 | 4 |
CdCu2GeS4 (mp-13982) | 0.2049 | 0.000 | 4 |
ZnP2 (mp-2782) | 0.3662 | 0.000 | 2 |
ZnP2 (mp-680550) | 0.4363 | 0.188 | 2 |
ZnP2 (mp-11025) | 0.3677 | 0.000 | 2 |
FeO (mp-781777) | 0.3971 | 0.085 | 2 |
ZnP2 (mp-1392) | 0.4087 | 0.003 | 2 |
Si (mp-971662) | 0.5574 | 0.063 | 1 |
Si (mp-1079297) | 0.5433 | 0.071 | 1 |
C (mp-1078845) | 0.4490 | 0.265 | 1 |
C (mp-1080826) | 0.4789 | 0.298 | 1 |
Si (mp-1095269) | 0.5478 | 0.090 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn Ga_d N O |
Final Energy/Atom-5.6855 eV |
Corrected Energy-184.7454 eV
-184.7454 eV = -181.9362 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)