Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.957 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.358 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 0 0> | <1 0 0> | 226.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 226.8 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 314.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 199.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 136.1 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 200.5 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 181.4 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 199.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 136.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 272.1 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 133.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 226.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 188.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 272.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 138.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 317.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 231.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 277.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 138.8 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 66.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 231.3 |
BN (mp-984) | <1 0 1> | <1 1 1> | 100.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 136.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 226.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 136.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 90.7 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 266.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 251.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 314.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 224.9 |
Al (mp-134) | <1 1 1> | <1 1 1> | 200.5 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 272.1 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 1> | 332.8 |
TeO2 (mp-2125) | <1 1 0> | <1 0 1> | 199.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 323.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 224.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 200.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 136.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 -1> | 188.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 272.1 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 199.7 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 266.3 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 317.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 314.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 323.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 231.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 231.3 |
BN (mp-984) | <1 1 0> | <1 0 0> | 136.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 188.8 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 -1> | 314.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.08 | 0.00 | 0.00 |
0.00 | 3.04 | 0.00 |
0.00 | 0.00 | 2.62 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.73 | 0.00 | -0.27 |
0.00 | 12.28 | 0.00 |
-0.27 | 0.00 | 6.64 |
Polycrystalline dielectric constant
εpoly∞
2.91
|
Polycrystalline dielectric constant
εpoly
10.21
|
Refractive Index n1.71 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbCr3O8 (mp-31753) | 0.3658 | 0.000 | 3 |
TlCr3O8 (mp-565782) | 0.3394 | 0.000 | 3 |
KCr3O8 (mp-19335) | 0.4664 | 0.000 | 3 |
CsTa(PO4)2 (mp-559118) | 0.1680 | 0.000 | 4 |
BaHf(PO4)2 (mp-545548) | 0.3828 | 0.000 | 4 |
CsNb(PO4)2 (mp-555286) | 0.1341 | 0.000 | 4 |
BaGe(PO4)2 (mp-1095485) | 0.4664 | 0.000 | 4 |
BaZr(PO4)2 (mp-556139) | 0.4268 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Ta_pv P O |
Final Energy/Atom-7.7590 eV |
Corrected Energy-98.6045 eV
Uncorrected energy = -93.1085 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Corrected energy = -98.6045 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)