Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.040 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.140 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 301.9 |
AlN (mp-661) | <0 0 1> | <1 1 -1> | 178.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 198.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 202.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 132.0 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 303.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 152.8 |
GaAs (mp-2534) | <1 0 0> | <1 1 -1> | 267.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 330.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 301.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 76.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 297.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 297.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 152.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 165.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 241.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 252.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 220.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 330.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 229.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 252.8 |
ZnSe (mp-1190) | <1 0 0> | <1 1 -1> | 267.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 241.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 229.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 198.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 363.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 231.0 |
LiF (mp-1138) | <1 0 0> | <1 1 -1> | 267.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 303.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 198.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 363.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 201.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 132.0 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 305.5 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 301.9 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 252.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 264.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 264.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 152.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 76.4 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 202.2 |
GaSe (mp-1943) | <1 1 0> | <1 0 1> | 229.1 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 231.0 |
BN (mp-984) | <0 0 1> | <1 0 1> | 76.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 231.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 165.0 |
BN (mp-984) | <1 1 0> | <0 1 1> | 301.9 |
BN (mp-984) | <1 1 1> | <1 1 1> | 274.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 99.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 165.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAgF4 (mp-765559) | 0.3163 | 0.000 | 3 |
LiFeF4 (mp-777801) | 0.3766 | 0.051 | 3 |
LiVF4 (mp-776493) | 0.3905 | 0.075 | 3 |
LiCu2F5 (mp-757119) | 0.5661 | 0.082 | 3 |
LiAuF4 (mp-12263) | 0.2484 | 0.004 | 3 |
YRe(WO4)2 (mvc-664) | 0.6964 | 0.265 | 4 |
MnO2 (mvc-14931) | 0.6586 | 0.206 | 2 |
SnO2 (mvc-6071) | 0.5766 | 0.305 | 2 |
NiO2 (mvc-6477) | 0.7151 | 0.337 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Au F |
Final Energy/Atom-3.8508 eV |
Corrected Energy-92.4193 eV
-92.4193 eV = -92.4193 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)