Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.289 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.337 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 300.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 300.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 300.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 214.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 343.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 280.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 171.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 171.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 300.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 257.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 300.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 257.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 43.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 214.8 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 300.7 |
Te2W (mp-22693) | <1 0 1> | <0 1 1> | 102.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 93.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 214.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 300.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 214.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 300.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 128.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 102.8 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 219.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 128.9 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 300.7 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 93.4 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 219.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 300.7 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 257.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 93.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 257.8 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 280.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 171.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 214.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 186.8 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 205.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 343.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 280.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 343.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 214.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 85.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 100.7 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 280.2 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 128.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 300.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 128.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 343.7 |
Al (mp-134) | <1 1 0> | <0 0 1> | 257.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 93.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.00000 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.13 | 0.00 | 0.00 |
0.00 | 3.22 | 0.00 |
0.00 | 0.00 | 3.38 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.47 | 0.00 | 0.00 |
0.00 | 9.30 | 0.00 |
0.00 | 0.00 | 10.95 |
Polycrystalline dielectric constant
εpoly∞
3.24
|
Polycrystalline dielectric constant
εpoly
10.24
|
Refractive Index n1.80 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd2(MoO4)3 (mp-650449) | 0.6775 | 0.000 | 3 |
Eu2Si2O7 (mp-21599) | 0.6595 | 0.045 | 3 |
Gd2(MoO4)3 (mp-554558) | 0.6782 | 0.000 | 3 |
Tb2(MoO4)3 (mp-19534) | 0.6779 | 0.000 | 3 |
Gd2Si2O7 (mp-13775) | 0.6725 | 0.000 | 3 |
NaY(SiO3)2 (mp-560039) | 0.5201 | 0.007 | 4 |
Er3Si3O10F (mp-542038) | 0.7202 | 0.006 | 4 |
Dy3Si3O10F (mp-16164) | 0.7166 | 0.000 | 4 |
Ho3Si3O10F (mp-16165) | 0.7169 | 0.000 | 4 |
Y3Si3O10F (mp-14630) | 0.7093 | 0.012 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Zr_sv P O |
Final Energy/Atom-7.9005 eV |
Corrected Energy-401.2083 eV
Uncorrected energy = -379.2243 eV
Composition-based energy adjustment (-0.687 eV/atom x 32.0 atoms) = -21.9840 eV
Corrected energy = -401.2083 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)