Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.358 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.288 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 236.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 163.2 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 138.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 236.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 163.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 289.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 289.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 224.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 224.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 122.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 122.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 280.1 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 208.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 289.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 285.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 122.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 209.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 326.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 163.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 326.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 204.0 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 289.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 163.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 139.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 277.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 69.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 285.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 139.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 122.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 224.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 244.8 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 104.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 104.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 69.9 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 168.1 |
TePb (mp-19717) | <1 1 1> | <1 1 0> | 289.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 204.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 204.0 |
BN (mp-984) | <1 0 0> | <1 1 -1> | 268.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 326.4 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 236.2 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 69.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 285.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 163.2 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 285.6 |
TiO2 (mp-2657) | <1 0 0> | <1 1 -1> | 179.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 280.1 |
TiO2 (mp-2657) | <1 1 1> | <0 1 1> | 207.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 204.0 |
C (mp-66) | <1 1 0> | <0 1 1> | 277.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2SiO4 (mp-4180) | 0.2854 | 0.035 | 3 |
Sr2GeO4 (mp-542085) | 0.3227 | 0.000 | 3 |
Ba2CoO4 (mp-19625) | 0.1372 | 0.000 | 3 |
Ba2TiO4 (mp-3397) | 0.1498 | 0.000 | 3 |
Sr2SiO4 (mp-18510) | 0.0634 | 0.000 | 3 |
KSrVO4 (mp-628859) | 0.3355 | 0.000 | 4 |
SrTlPS4 (mp-17090) | 0.3732 | 0.000 | 4 |
SrTlVO4 (mp-566556) | 0.3489 | 0.000 | 4 |
NaNdSiO4 (mp-13774) | 0.3516 | 0.000 | 4 |
NaLaSiO4 (mp-1020648) | 0.3373 | 0.000 | 4 |
InI2 (mp-29312) | 0.6538 | 0.000 | 2 |
InBr2 (mp-568108) | 0.7139 | 0.000 | 2 |
GaBr2 (mp-650841) | 0.5492 | 0.011 | 2 |
GaCl2 (mp-568848) | 0.6968 | 0.000 | 2 |
GaBr2 (mp-28384) | 0.6767 | 0.000 | 2 |
SrLaTl(AsO4)2 (mp-685195) | 0.5245 | 0.000 | 5 |
KBiS(ClO2)2 (mp-23645) | 0.5075 | 0.000 | 5 |
KSnSO4F (mp-557399) | 0.5140 | 0.000 | 5 |
K2YbMoPO8 (mp-565817) | 0.5222 | 0.000 | 5 |
K2BiPWO8 (mp-566769) | 0.5311 | 0.001 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Eu Si O |
Final Energy/Atom-9.4999 eV |
Corrected Energy-277.2337 eV
-277.2337 eV = -265.9971 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|