material

RbCuF3

ID:

mp-554601


Material Details

Final Magnetic Moment
1.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.346 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.008 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.82 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
RbCuF3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdSe (mp-2691) <1 0 0> <1 0 0> 0.000 154.3
CdSe (mp-2691) <1 1 0> <1 1 0> 0.000 218.3
GaSb (mp-1156) <1 0 0> <1 0 0> 0.002 154.3
GaSb (mp-1156) <1 1 0> <1 1 0> 0.002 218.3
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.003 137.2
Si (mp-149) <1 1 1> <1 1 1> 0.004 207.9
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.005 207.9
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.006 154.3
PbSe (mp-2201) <1 0 0> <1 0 0> 0.007 154.3
PbSe (mp-2201) <1 1 0> <1 1 0> 0.008 218.3
TePb (mp-19717) <1 0 0> <1 0 0> 0.010 85.7
SiC (mp-8062) <1 0 0> <1 0 0> 0.011 154.3
SiC (mp-11714) <1 1 0> <1 1 0> 0.011 218.3
SiC (mp-8062) <1 1 0> <1 1 0> 0.011 218.3
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.012 222.9
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.013 137.2
C (mp-66) <1 1 0> <1 1 0> 0.014 72.8
C (mp-66) <1 1 1> <1 1 1> 0.014 89.1
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.017 154.3
Te2W (mp-22693) <0 1 1> <1 1 0> 0.017 291.0
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.018 72.8
SiC (mp-11714) <1 0 0> <1 1 0> 0.019 218.3
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.020 89.1
Mg (mp-153) <1 1 1> <1 0 0> 0.022 274.4
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.023 154.3
GaSe (mp-1943) <0 0 1> <1 1 1> 0.025 89.1
BN (mp-984) <1 0 0> <1 0 0> 0.025 291.5
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.025 308.7
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.025 218.3
GaN (mp-804) <1 1 1> <1 0 0> 0.027 274.4
Ag (mp-124) <1 0 0> <1 0 0> 0.027 17.1
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.028 85.7
Ag (mp-124) <1 1 0> <1 1 0> 0.029 24.3
Ag (mp-124) <1 1 1> <1 1 1> 0.030 29.7
InAs (mp-20305) <1 0 0> <1 0 0> 0.030 154.3
InAs (mp-20305) <1 1 0> <1 1 0> 0.032 218.3
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.035 118.8
GaP (mp-2490) <1 1 1> <1 1 1> 0.035 207.9
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.036 266.8
C (mp-48) <1 1 1> <1 1 0> 0.038 169.8
C (mp-48) <0 0 1> <1 1 1> 0.042 207.9
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.043 218.3
SiC (mp-11714) <1 0 1> <1 0 0> 0.047 257.2
AlN (mp-661) <0 0 1> <1 1 0> 0.048 169.8
GdScO3 (mp-5690) <1 0 1> <1 1 0> 0.054 169.8
AlN (mp-661) <1 1 0> <1 1 0> 0.055 218.3
TiO2 (mp-390) <1 0 0> <1 0 0> 0.056 257.2
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.061 207.9
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.064 154.3
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.064 207.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
94 50 50 0 0 0
50 94 50 0 0 0
50 50 94 0 0 0
0 0 0 37 0 0
0 0 0 0 37 0
0 0 0 0 0 37
Compliance Tensor Sij (10-12Pa-1)
16.7 -5.8 -5.8 -0.0 0.0 0.0
-5.8 16.7 -5.8 0.0 -0.0 0.0
-5.8 -5.8 16.7 -0.0 0.0 -0.0
-0.0 0.0 -0.0 27.0 -0.0 0.0
0.0 -0.0 0.0 -0.0 27.0 -0.0
0.0 0.0 -0.0 0.0 -0.0 27.0
Shear Modulus GV
31 GPa
Bulk Modulus KV
64 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
64 GPa
Shear Modulus GVRH
30 GPa
Bulk Modulus KVRH
64 GPa
Elastic Anisotropy
0.32
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CaSnO3 (mp-546910) 0.0019 1.494 3
TiPbO3 (mp-19845) 0.0019 0.041 3
KCrF3 (mp-601328) 0.0018 0.082 3
LaFeO3 (mp-556561) 0.0018 0.130 3
SrMoO3 (mp-1068267) 0.0018 0.087 3
La2ReNiO6 (mp-1078601) 0.0037 0.288 4
Cs2LiYCl6 (mp-567652) 0.0021 0.000 4
Sr2GaSbO6 (mp-6065) 0.0032 0.039 4
Ba2YbSbO6 (mp-14223) 0.0037 1.747 4
Ba2NbFeO6 (mp-1096853) 0.0037 2.749 4
Nd2O3 (mp-33029) 0.0037 0.929 2
La2O3 (mp-33032) 0.0037 0.891 2
Fe4P (mp-20885) 0.0026 0.686 2
Ni4O (mp-1094082) 0.0037 1.732 2
Ni4N (mp-1094090) 0.0037 0.067 2
BaLaMgBiO6 (mp-41414) 0.0488 0.096 5
BaLaMgNbO6 (mp-39288) 0.0711 0.090 5
SrLaNbZnO6 (mp-41918) 0.0665 0.126 5
SrLaMnCoO6 (mp-40761) 0.0404 0.247 5
Sr6Ca2MnFe7O24 (mp-1075969) 0.0467 0.021 5
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) 0.7370 0.065 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Rb_sv Cu_pv F
Final Energy/Atom
-4.2147 eV
Corrected Energy
-22.4597 eV
Uncorrected energy = -21.0737 eV Composition-based energy adjustment (-0.462 eV/atom x 3.0 atoms) = -1.3860 eV Corrected energy = -22.4597 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)