Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.533 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.580 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 1> | 293.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 98.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 266.1 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 195.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 319.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 319.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 246.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 164.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 293.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 319.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 212.9 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 143.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 319.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 159.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 319.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 195.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 98.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 98.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 159.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 159.7 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 246.7 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 246.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 319.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 266.1 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 293.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 293.9 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 212.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 266.1 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 98.0 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 293.9 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 143.6 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 133.4 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 266.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 159.7 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 266.1 |
TeO2 (mp-2125) | <0 0 1> | <0 1 1> | 98.0 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 212.9 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 133.4 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 266.1 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 293.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 266.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 159.7 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 1> | 195.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 0> | 156.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 246.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 246.7 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 246.7 |
Al (mp-134) | <1 0 0> | <0 1 1> | 98.0 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 319.4 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 164.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.10237 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.16894 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00988 |
Piezoelectric Modulus ‖eij‖max0.16894 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.33 | 0.00 | 0.00 |
0.00 | 2.44 | 0.00 |
0.00 | 0.00 | 2.45 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.85 | 0.00 | 0.00 |
0.00 | 9.91 | 0.00 |
0.00 | 0.00 | 9.10 |
Polycrystalline dielectric constant
εpoly∞
2.40
|
Polycrystalline dielectric constant
εpoly
10.29
|
Refractive Index n1.55 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2MnO4 (mp-772365) | 0.6599 | 0.006 | 3 |
K2CrO4 (mp-775274) | 0.6839 | 0.016 | 3 |
U3(PO9)2 (mp-863013) | 0.7407 | 0.524 | 3 |
Tl2PS3 (mp-28217) | 0.7215 | 0.000 | 3 |
K3Sm(PO4)2 (mp-18019) | 0.6043 | 0.000 | 4 |
Rb2U2Mo3O16 (mp-687091) | 0.5892 | 0.003 | 4 |
U2Tl2Mo3O16 (mp-641191) | 0.6022 | 0.001 | 4 |
K3Eu(PO4)2 (mp-17089) | 0.6123 | 0.237 | 4 |
K3Nd(PO4)2 (mp-17187) | 0.6086 | 0.000 | 4 |
K2USO7F2 (mp-863004) | 0.6961 | 0.185 | 5 |
BaNaNdSi2O7 (mp-559384) | 0.7202 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Sb S O F |
Final Energy/Atom-5.3571 eV |
Corrected Energy-249.6013 eV
-249.6013 eV = -235.7108 eV (uncorrected energy) - 13.8905 eV (MP Anion Correction)
|