Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.431 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTiO2 + Ti3O5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 308.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 191.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 229.4 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 247.2 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 255.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 114.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 1> | 123.6 |
CeO2 (mp-20194) | <1 1 1> | <1 1 -1> | 256.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 191.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 273.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 267.7 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 185.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 153.0 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 192.3 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 203.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 191.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 287.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 203.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 254.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 191.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 256.4 |
KCl (mp-23193) | <1 0 0> | <0 1 -1> | 273.2 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 232.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 191.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 152.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 344.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 -1> | 267.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 230.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 273.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 1> | 278.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 232.4 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 318.8 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 256.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 267.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 222.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 191.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 203.2 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 114.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 153.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 76.5 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 203.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 344.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 232.4 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 254.0 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 254.0 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 304.8 |
Te2W (mp-22693) | <0 1 0> | <1 -1 0> | 165.4 |
Te2W (mp-22693) | <1 1 0> | <1 0 -1> | 222.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 172.7 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 139.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2SiO5 (mp-9515) | 0.3039 | 0.100 | 3 |
Nb2(CoO3)3 (mvc-13231) | 0.3345 | 0.239 | 3 |
TiGa2O5 (mp-752733) | 0.3440 | 0.077 | 3 |
CrFe2O5 (mp-769927) | 0.3066 | 0.802 | 3 |
TiFe2O5 (mp-19255) | 0.2992 | 0.638 | 3 |
Li2Fe2OF6 (mp-777626) | 0.3058 | 0.474 | 4 |
LiV6O7F5 (mp-777058) | 0.3236 | 0.097 | 4 |
Li3Nb3TeO12 (mp-754751) | 0.3539 | 0.018 | 4 |
Ta2TiZn2O8 (mvc-2345) | 0.3059 | 0.159 | 4 |
TiNb2Zn2O8 (mvc-3345) | 0.3017 | 0.120 | 4 |
Ti9O17 (mp-27273) | 0.1957 | 0.016 | 2 |
Ti6O11 (mp-30524) | 0.1302 | 0.012 | 2 |
Ti5O9 (mp-748) | 0.0212 | 0.011 | 2 |
Ti7O13 (mp-556724) | 0.1386 | 0.013 | 2 |
Ti6O11 (mp-680568) | 0.1417 | 0.012 | 2 |
Li4CrSb(WO6)2 (mp-764950) | 0.4131 | 0.036 | 5 |
Li4FeTe(WO6)2 (mp-771716) | 0.3833 | 0.163 | 5 |
Li4MnSb2WO12 (mp-763536) | 0.4308 | 0.067 | 5 |
Li4CrTe(WO6)2 (mp-777147) | 0.4306 | 0.168 | 5 |
Li4FeSb(WO6)2 (mp-767012) | 0.4168 | 3.405 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv O |
Final Energy/Atom-8.9802 eV |
Corrected Energy-264.0862 eV
-264.0862 eV = -251.4450 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)