Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.006 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.046 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 322.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 282.3 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 215.0 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 169.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 215.0 |
GaAs (mp-2534) | <1 1 0> | <0 1 -1> | 279.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 -1> | 274.0 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 198.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 215.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 319.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 282.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 322.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 232.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 206.6 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 274.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 169.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 215.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 87.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 268.8 |
TePb (mp-19717) | <1 0 0> | <1 -1 0> | 216.7 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 167.9 |
AlN (mp-661) | <1 0 1> | <1 -1 1> | 182.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 261.0 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 323.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 264.5 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 186.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 169.4 |
GaN (mp-804) | <1 0 1> | <1 -1 -1> | 186.2 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 261.5 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 215.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 268.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 215.0 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 161.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 0> | 162.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 0> | 216.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 58.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 0> | 162.5 |
CdS (mp-672) | <1 0 1> | <1 -1 0> | 162.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 348.1 |
Al (mp-134) | <1 0 0> | <1 -1 1> | 182.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 169.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 -1 0> | 270.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 -1 1> | 243.4 |
LiF (mp-1138) | <1 1 0> | <1 -1 0> | 162.5 |
CdTe (mp-406) | <1 0 0> | <1 -1 0> | 216.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 268.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 261.0 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 269.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 87.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
As(IF3)2 (mp-558244) | 0.5484 | 0.000 | 3 |
BaSb2F12 (mp-861962) | 0.4167 | 0.004 | 3 |
Ir(Cl2F3)2 (mp-29870) | 0.5234 | 0.000 | 3 |
Rh(OF3)2 (mp-19790) | 0.5138 | 0.000 | 3 |
As2HPbF13 (mp-758957) | 0.5046 | 0.000 | 4 |
SbSNF6 (mp-683956) | 0.3978 | 0.103 | 4 |
TeAs(BrF2)3 (mp-557570) | 0.5141 | 0.026 | 4 |
AsS(IF3)2 (mp-557628) | 0.5258 | 0.000 | 4 |
AsSe(ClF2)3 (mp-554706) | 0.5198 | 0.000 | 4 |
VF5 (mp-764952) | 0.6927 | 0.004 | 2 |
BiF5 (mvc-3518) | 0.6571 | 0.003 | 2 |
UF6 (mp-672341) | 0.6076 | 0.004 | 2 |
SbF4 (mp-556425) | 0.4795 | 0.000 | 2 |
VF5 (mp-765218) | 0.7043 | 0.013 | 2 |
Sb2RuC6(OF2)6 (mp-6891) | 0.7466 | 0.091 | 5 |
Sb2OsC6(OF2)6 (mp-6880) | 0.7452 | 0.077 | 5 |
HgSb4C2(OF11)2 (mp-556903) | 0.6633 | 0.081 | 5 |
Sb4OsC6(O3F11)2 (mp-558754) | 0.7413 | 0.083 | 5 |
Sb4RuC6(O3F11)2 (mp-555952) | 0.7429 | 0.092 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Sb F |
Final Energy/Atom-4.8213 eV |
Corrected Energy-72.3192 eV
-72.3192 eV = -72.3192 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)