Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.983 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.016 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoBr2 + MoS2 |
Band Gap0.895 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 176.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 143.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 203.3 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 143.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 203.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 143.7 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 176.0 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 176.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 101.6 |
C (mp-66) | <1 1 0> | <1 1 0> | 143.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 176.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 101.6 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 101.6 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 143.7 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 176.0 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 143.7 |
Ge (mp-32) | <1 1 1> | <1 1 1> | 176.0 |
Fe2O3 (mp-24972) | <1 0 0> | <1 1 0> | 143.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
84 | 42 | 42 | 0 | 0 | 0 |
42 | 84 | 42 | 0 | 0 | 0 |
42 | 42 | 84 | 0 | 0 | 0 |
0 | 0 | 0 | 36 | 0 | 0 |
0 | 0 | 0 | 0 | 36 | 0 |
0 | 0 | 0 | 0 | 0 | 36 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
17.9 | -6.0 | -6.0 | -0.0 | 0.0 | 0.0 |
-6.0 | 17.9 | -6.0 | 0.0 | -0.0 | 0.0 |
-6.0 | -6.0 | 17.9 | 0.0 | 0.0 | -0.0 |
-0.0 | 0.0 | 0.0 | 27.7 | 0.0 | 0.0 |
0.0 | -0.0 | 0.0 | 0.0 | 27.7 | 0.0 |
0.0 | 0.0 | -0.0 | 0.0 | 0.0 | 27.7 |
Shear Modulus GV30 GPa |
Bulk Modulus KV56 GPa |
Shear Modulus GR28 GPa |
Bulk Modulus KR56 GPa |
Shear Modulus GVRH29 GPa |
Bulk Modulus KVRH56 GPa |
Elastic Anisotropy0.37 |
Poisson's Ratio0.28 |
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.20328 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.20328 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.20328 |
Piezoelectric Modulus ‖eij‖max0.20328 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
8.33 | 0.00 | 0.00 |
0.00 | 8.33 | 0.00 |
0.00 | 0.00 | 8.33 |
Dielectric Tensor εij (total) |
||
---|---|---|
8.93 | 0.00 | 0.00 |
0.00 | 8.93 | 0.00 |
0.00 | 0.00 | 8.93 |
Polycrystalline dielectric constant
εpoly∞
8.33
|
Polycrystalline dielectric constant
εpoly
8.93
|
Refractive Index n2.89 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaGeI (mp-568574) | 0.7072 | 0.000 | 3 |
ReTeS (mp-5222) | 0.0734 | 0.000 | 3 |
TbGaI (mp-1025099) | 0.7236 | 0.000 | 3 |
NbSeI (mp-23051) | 0.0326 | 0.000 | 3 |
MoS2 (mvc-11780) | 0.4880 | 0.268 | 2 |
TcS2 (mp-9481) | 0.6882 | 0.000 | 2 |
ReS2 (mp-572758) | 0.6710 | 0.000 | 2 |
PrI2 (mp-569673) | 0.7074 | 0.000 | 2 |
ReSe2 (mp-541582) | 0.6807 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mo_pv S Br |
Final Energy/Atom-6.3015 eV |
Corrected Energy-78.2721 eV
-78.2721 eV = -75.6182 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)