Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.013 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb2PS10 + NbS2 + Ag2S + Ag3PS4 |
Band Gap1.443 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2Ge2Se5 (mp-18335) | 0.7076 | 0.000 | 3 |
Ba3Sn2S7 (mp-556291) | 0.7214 | 0.000 | 3 |
Dy4(SiS4)3 (mp-10771) | 0.7075 | 0.002 | 3 |
Ag2PSe3 (mp-13956) | 0.7171 | 0.000 | 3 |
Tb4(SiS4)3 (mp-16402) | 0.7221 | 0.000 | 3 |
RbNb2PS10 (mp-6708) | 0.6328 | 0.000 | 4 |
KNb2PS10 (mp-542972) | 0.5934 | 0.000 | 4 |
YAg3(PS4)2 (mp-561467) | 0.6519 | 0.000 | 4 |
NbAg2(PS4)2 (mp-554336) | 0.5389 | 0.012 | 4 |
Nb2TlPS10 (mp-560847) | 0.4891 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Ag P S |
Final Energy/Atom-5.5253 eV |
Corrected Energy-335.9572 eV
-335.9572 eV = -309.4188 eV (uncorrected energy) - 26.5384 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)