Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.874 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSbSCl9 + SCl + SbCl3 + N2 |
Band Gap1.784 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImmm [71] |
Hall-I 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 107.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 297.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.3 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 107.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 297.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 214.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 178.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 238.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 238.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 297.9 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 93.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 297.9 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 214.0 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 100.0 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 71.3 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 214.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 93.0 |
BN (mp-984) | <0 0 1> | <1 1 1> | 245.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 238.3 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 240.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 178.8 |
TeO2 (mp-2125) | <1 1 0> | <1 0 1> | 100.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 178.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 178.8 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 178.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 238.3 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 1> | 200.0 |
GdScO3 (mp-5690) | <1 1 1> | <1 1 0> | 214.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 238.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 238.3 |
LaF3 (mp-905) | <0 0 1> | <0 1 1> | 93.0 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 214.0 |
LaF3 (mp-905) | <1 0 1> | <1 1 0> | 214.9 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 100.0 |
InP (mp-20351) | <1 1 1> | <0 1 1> | 185.9 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 107.4 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 238.3 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 285.4 |
TbScO3 (mp-31119) | <1 1 1> | <1 1 0> | 214.9 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 240.9 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 1> | 100.0 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 297.9 |
NdGaO3 (mp-3196) | <0 1 1> | <1 1 0> | 107.4 |
NdGaO3 (mp-3196) | <1 1 1> | <1 1 0> | 214.9 |
WS2 (mp-224) | <0 0 1> | <0 1 1> | 185.9 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 238.3 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 238.3 |
C (mp-48) | <0 0 1> | <0 0 1> | 238.3 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 214.0 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 1 1> | 185.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
16 | 2 | 5 | 0 | 0 | 0 |
2 | 10 | 2 | 0 | 0 | 0 |
5 | 2 | 15 | 0 | 0 | 0 |
0 | 0 | 0 | 2 | 0 | 0 |
0 | 0 | 0 | 0 | 1 | 0 |
0 | 0 | 0 | 0 | 0 | 2 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
70.4 | -11.8 | -23.9 | -0.0 | 0.0 | -0.0 |
-11.8 | 108.6 | -12.2 | 0.0 | -0.0 | -0.0 |
-23.9 | -12.2 | 79.3 | 0.0 | 0.0 | 0.0 |
-0.0 | 0.0 | 0.0 | 542.1 | 0.0 | 0.0 |
0.0 | -0.0 | 0.0 | 0.0 | 974.1 | 0.0 |
-0.0 | -0.0 | 0.0 | 0.0 | 0.0 | 448.0 |
Shear Modulus GV3 GPa |
Bulk Modulus KV7 GPa |
Shear Modulus GR2 GPa |
Bulk Modulus KR6 GPa |
Shear Modulus GVRH3 GPa |
Bulk Modulus KVRH6 GPa |
Elastic Anisotropy2.38 |
Poisson's Ratio0.32 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V(CO)6 (mp-647985) | 0.5160 | 0.557 | 3 |
AsN2F7 (mp-685810) | 0.4181 | 0.000 | 3 |
WOF4 (mp-540636) | 0.4798 | 0.010 | 3 |
WN3F5 (mp-558743) | 0.4419 | 0.125 | 3 |
ReNF6 (mp-28012) | 0.4034 | 0.222 | 3 |
AsS2NF6 (mp-8500) | 0.3618 | 0.025 | 4 |
CSNF5 (mp-562018) | 0.4151 | 0.469 | 4 |
SbCNCl6 (mp-570727) | 0.3512 | 0.075 | 4 |
SbS2NF6 (mp-12368) | 0.3801 | 0.009 | 4 |
SbN(OF3)2 (mp-1078298) | 0.4309 | 0.000 | 4 |
TaF5 (mp-561197) | 0.6792 | 0.000 | 2 |
BiF5 (mp-27743) | 0.6169 | 0.000 | 2 |
MoF5 (mp-555649) | 0.6453 | 0.078 | 2 |
UO5 (mp-1072461) | 0.6662 | 0.580 | 2 |
MoF5 (mp-608126) | 0.6431 | 0.078 | 2 |
Sb2RuC6(OF2)6 (mp-6891) | 0.5648 | 0.091 | 5 |
Sb2OsC6(OF2)6 (mp-6880) | 0.5664 | 0.078 | 5 |
Te6As4C3(NF8)3 (mp-555419) | 0.5822 | 0.193 | 5 |
ZnAs2C12(NF)12 (mp-555971) | 0.4603 | 0.318 | 5 |
FeSb2C6(OF2)6 (mp-19466) | 0.5435 | 0.309 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb S N Cl |
Final Energy/Atom-3.5294 eV |
Corrected Energy-39.9844 eV
Uncorrected energy = -35.2944 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.614 eV/atom x 6.0 atoms) = -3.6840 eV
Corrected energy = -39.9844 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)