Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.144 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.548 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 221.4 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 199.4 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 199.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 199.4 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 221.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 221.4 |
WSe2 (mp-1821) | <1 0 0> | <1 0 -1> | 199.4 |
WSe2 (mp-1821) | <1 1 0> | <1 0 0> | 177.6 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 0> | 221.4 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 177.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pr9Be4O20 (mp-675648) | 0.6159 | 0.108 | 3 |
Rb3ZnBr5 (mp-505001) | 0.6299 | 0.003 | 3 |
Ba3FeO5 (mp-505787) | 0.5056 | 0.004 | 3 |
Ba2CoO4 (mp-19625) | 0.6170 | 0.000 | 3 |
K2SeO4 (mp-557025) | 0.6266 | 0.000 | 3 |
Eu5Si(Cl3O2)2 (mp-669318) | 0.1838 | 0.000 | 4 |
Sm2SiTeO4 (mp-17812) | 0.5424 | 0.007 | 4 |
Nd2SiTeO4 (mp-17959) | 0.5188 | 0.007 | 4 |
Ba5Si(Br3O2)2 (mp-553884) | 0.2039 | 0.000 | 4 |
Pr2SiTeO4 (mp-541996) | 0.4942 | 0.006 | 4 |
GaBr2 (mp-650841) | 0.7265 | 0.011 | 2 |
Na3Pb2S3ClO12 (mp-677013) | 0.6289 | 0.000 | 5 |
KBiS(ClO2)2 (mp-23645) | 0.7221 | 0.000 | 5 |
NaPr9Si6(SO12)2 (mp-686572) | 0.6147 | 0.000 | 5 |
NaSm9Si6(SO12)2 (mp-686543) | 0.6471 | 0.000 | 5 |
CaGdTh(PO4)3 (mp-695308) | 0.6895 | 0.013 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Si Cl O |
Final Energy/Atom-5.6140 eV |
Corrected Energy-185.2657 eV
-185.2657 eV = -179.6474 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)