Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.115 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNdSBr + NdBr3 |
Band Gap2.818 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 299.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 199.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 249.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 349.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 299.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 299.7 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 299.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 299.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 199.8 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 49.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 249.7 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 349.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 149.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 149.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 349.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 349.6 |
BN (mp-984) | <1 0 0> | <1 0 0> | 349.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 299.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 349.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 299.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 149.8 |
Al (mp-134) | <1 1 0> | <1 0 0> | 199.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 349.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 299.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 349.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 349.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 249.7 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 349.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 149.8 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 299.7 |
C (mp-66) | <1 1 0> | <1 0 0> | 199.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 149.8 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 299.7 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 49.9 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 249.7 |
C (mp-48) | <1 0 0> | <1 0 0> | 349.6 |
C (mp-48) | <1 0 1> | <1 0 0> | 349.6 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 0> | 349.6 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 349.6 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 249.7 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 349.6 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 299.7 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 249.7 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 0> | 249.7 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 299.7 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 349.6 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 349.6 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 149.8 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 349.6 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 199.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd2SCl4 (mp-865182) | 0.4182 | 0.000 | 3 |
Sm2SCl4 (mp-29880) | 0.4842 | 0.000 | 3 |
Dy3S2Cl5 (mp-30157) | 0.4556 | 0.020 | 3 |
Nd3S2Cl5 (mp-556023) | 0.4767 | 0.000 | 3 |
Nd3S2Br5 (mp-28297) | 0.2808 | 0.020 | 3 |
SrHg2(ClO)2 (mp-554351) | 0.6990 | 0.000 | 4 |
Nb2Tl3CuSe12 (mp-570757) | 0.7347 | 0.000 | 4 |
Ba2V(CuS2)3 (mp-560493) | 0.6873 | 0.038 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.7491 | 0.000 | 4 |
Sm5Co2 (mp-7317) | 0.5930 | 0.000 | 2 |
Ca5Au2 (mp-30367) | 0.4414 | 0.000 | 2 |
Dy5Ru2 (mp-30622) | 0.4788 | 0.000 | 2 |
B2Pd5 (mp-2617) | 0.6415 | 0.006 | 2 |
Sr7Pt3 (mp-30843) | 0.5533 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 S Br |
Final Energy/Atom-5.1389 eV |
Corrected Energy-143.0378 eV
Uncorrected energy = -133.6118 eV
Composition-based energy adjustment (-0.503 eV/atom x 6.0 atoms) = -3.0180 eV
Composition-based energy adjustment (-0.534 eV/atom x 12.0 atoms) = -6.4080 eV
Corrected energy = -143.0378 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)