Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.275 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.511 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 260.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 225.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 315.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 300.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 225.2 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 131.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 45.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 225.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 315.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 315.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 225.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 75.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 260.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 300.3 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 260.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 262.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 225.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 270.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 270.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 270.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 90.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 135.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 90.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 315.6 |
BN (mp-984) | <1 0 1> | <0 1 0> | 218.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 135.2 |
BN (mp-984) | <1 1 1> | <0 0 1> | 135.2 |
Al (mp-134) | <1 1 1> | <1 1 1> | 197.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 225.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 174.8 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 313.9 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 300.3 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 305.9 |
SiC (mp-7631) | <1 1 1> | <0 1 1> | 251.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 45.1 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 260.6 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 260.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 90.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 45.1 |
GdScO3 (mp-5690) | <1 1 1> | <1 1 1> | 296.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 270.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 180.3 |
Mg (mp-153) | <1 1 1> | <1 1 1> | 296.4 |
LaF3 (mp-905) | <1 1 1> | <1 1 1> | 98.8 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 349.7 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 180.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 315.6 |
Ni (mp-23) | <1 1 1> | <1 1 0> | 86.9 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 315.6 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 225.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-0.00199 | 0.02180 | -0.02099 | 0.00000 | 0.00983 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.11759 | 0.00000 | -0.06479 |
0.06585 | 0.12541 | -0.07152 | 0.00000 | 0.08345 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.18139 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
6.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.17 | 0.00 | 0.00 |
0.00 | 2.16 | 0.00 |
0.00 | 0.00 | 2.16 |
Dielectric Tensor εij (total) |
||
---|---|---|
3.96 | 0.00 | 0.08 |
0.00 | 3.86 | 0.00 |
0.08 | 0.00 | 3.88 |
Polycrystalline dielectric constant
εpoly∞
2.17
|
Polycrystalline dielectric constant
εpoly
3.90
|
Refractive Index n1.47 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5724) | 0.3257 | 0.003 | 3 |
AlPO4 (mp-5859) | 0.3093 | 0.011 | 3 |
AlPO4 (mp-37990) | 0.3474 | 0.014 | 3 |
AlPO4 (mp-557362) | 0.3674 | 0.010 | 3 |
AlPO4 (mp-557842) | 0.3544 | 0.011 | 3 |
CsAlSiO4 (mp-561457) | 0.6793 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.5820 | 0.000 | 4 |
SiO2 (mp-8059) | 0.1276 | 0.005 | 2 |
SiO2 (mp-542814) | 0.0985 | 0.004 | 2 |
SiO2 (mp-15078) | 0.1251 | 0.012 | 2 |
CrN2 (mp-1097039) | 0.1447 | 0.371 | 2 |
CrN2 (mp-1096909) | 0.1332 | 0.361 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9129 eV |
Corrected Energy-100.5730 eV
-100.5730 eV = -94.9546 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)