Final Magnetic Moment0.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.044 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSb9S4F39 + SF4 + Sb2S19F12 + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2O2F9 (mp-504690) | 0.7479 | 0.000 | 3 |
Sb2N5F11 (mp-542148) | 0.7074 | 0.000 | 3 |
Sb9Se4F39 (mp-15380) | 0.7455 | 0.000 | 3 |
SbS5N5Cl6 (mp-647878) | 0.6940 | 0.161 | 4 |
Ba4Al3Cu2F21 (mp-553943) | 0.6907 | 0.004 | 4 |
GeClO2F5 (mp-557432) | 0.5575 | 0.000 | 4 |
SbS2NCl8 (mp-554625) | 0.5395 | 0.013 | 4 |
MgAs2(XeF5)4 (mp-555546) | 0.7221 | 0.000 | 4 |
CoSb2S2(OF3)4 (mp-629319) | 0.5975 | 0.001 | 5 |
CuAs2S4(O2F3)4 (mp-556926) | 0.6666 | 0.025 | 5 |
MgAs2S2(OF3)4 (mp-555121) | 0.5829 | 0.052 | 5 |
NiAs2S6(OF)12 (mp-566394) | 0.6287 | 0.020 | 5 |
MnAs2S2(OF3)4 (mp-562665) | 0.6087 | 0.040 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb S N F |
Final Energy/Atom-4.8763 eV |
Corrected Energy-634.7854 eV
-634.7854 eV = -624.1701 eV (uncorrected energy) - 10.6154 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)