Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-1.784 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.089 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrSO4 + MnO + SrS + Cu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Groupmmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 253.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 219.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 202.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 287.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 152.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 33.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 168.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 152.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 216.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 202.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 270.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 354.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 287.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 253.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 304.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 288.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 135.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 144.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 168.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 304.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 144.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 152.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 216.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 33.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 144.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 168.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 236.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 304.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 16.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 84.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 118.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 287.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 216.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 84.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 84.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 185.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 270.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 16.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 72.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 320.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 216.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 320.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 288.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 84.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 219.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 202.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 72.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 320.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 16.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr2Cu3(SO)2 (mp-7112) | 0.4568 | 0.130 | 4 |
Ba2Mn3(AsO)2 (mp-18963) | 0.4392 | 0.047 | 4 |
Ce2Fe2S2O3 (mp-1078984) | 0.3440 | 0.109 | 4 |
Pr2Fe2S2O3 (mp-1079573) | 0.3520 | 0.020 | 4 |
La2Co2Se2O3 (mp-1079800) | 0.4237 | 0.081 | 4 |
Sr2Fe2Se2OF2 (mp-557839) | 0.3504 | 0.000 | 5 |
Sr2Fe2S2OF2 (mp-561913) | 0.2117 | 0.000 | 5 |
Sr2ZnCu2(SO)2 (mp-9453) | 0.2215 | 0.082 | 5 |
Sr2MnZn2(AsO)2 (mp-863942) | 0.3453 | 0.000 | 5 |
Ba2Mn2Se2OF2 (mp-1080029) | 0.3860 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Sr_sv Mn_pv Cu_pv S O |
Final Energy/Atom-5.6166 eV |
Corrected Energy-109.9232 eV
-109.9232 eV = -101.0985 eV (uncorrected energy) - 5.4630 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)