Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.063 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.134 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2O + Li2CO3 |
Band Gap5.351 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmc21 [36] |
HallC 2c 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 158.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 298.4 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 241.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 215.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 215.2 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 241.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 242.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 241.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 242.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 341.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 213.1 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 204.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 211.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 121.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 264.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 204.0 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 298.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 68.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 127.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 170.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 242.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 121.1 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 60.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 121.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 170.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 264.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 298.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 255.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 264.9 |
BN (mp-984) | <1 1 0> | <1 1 0> | 242.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 211.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 127.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 264.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 170.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 170.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 213.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 211.9 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 204.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 341.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 211.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 160.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 53.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 136.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 211.9 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 298.4 |
Al (mp-134) | <1 1 0> | <0 1 0> | 213.1 |
Al (mp-134) | <1 1 1> | <0 1 0> | 298.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 241.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 273.0 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 213.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
-0.01245 | 0.11966 | 1.25825 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max1.26399 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.69 | 0.00 | 0.00 |
0.00 | 2.68 | 0.00 |
0.00 | 0.00 | 2.74 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.71 | 0.00 | 0.00 |
0.00 | 9.79 | 0.00 |
0.00 | 0.00 | 13.12 |
Polycrystalline dielectric constant
εpoly∞
2.70
|
Polycrystalline dielectric constant
εpoly
11.54
|
Refractive Index n1.64 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr3MoN4 (mp-31356) | 0.5447 | 0.004 | 3 |
K4TiO4 (mp-756510) | 0.5482 | 0.000 | 3 |
Sr7GeN6 (mp-568436) | 0.5400 | 0.000 | 3 |
Sr3MoN4 (mp-570046) | 0.5365 | 0.000 | 3 |
Ca7SiN6 (mp-1029474) | 0.5261 | 0.000 | 3 |
LiSiBi3O7 (mp-757777) | 0.6450 | 0.042 | 4 |
Na3VSO3 (mp-565254) | 0.6457 | 0.038 | 4 |
Pr3MnAlS7 (mp-867323) | 0.6379 | 0.000 | 4 |
Nd3MnAlS7 (mp-864652) | 0.6131 | 0.000 | 4 |
Sm3MnAlS7 (mp-867965) | 0.5946 | 0.000 | 4 |
Li5MnP2(O4F)2 (mp-762699) | 0.7440 | 0.041 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv C O |
Final Energy/Atom-5.8176 eV |
Corrected Energy-110.3354 eV
-110.3354 eV = -104.7171 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)