Final Magnetic Moment6.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.311 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.036 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKPd2O3 + K3(PdO2)2 + Gd2O3 + Pd |
Band Gap0.799 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 267.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 297.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 197.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 148.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 155.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 192.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 327.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 238.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 289.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 259.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 207.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 131.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 208.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 267.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 329.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 148.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 259.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 356.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 327.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 267.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 329.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 238.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 259.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 131.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 311.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 311.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 267.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 267.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 259.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 297.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 197.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 159.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 89.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 311.3 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 356.9 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 263.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 259.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 327.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 208.2 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 197.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 263.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 119.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 267.7 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 267.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 267.7 |
BN (mp-984) | <1 0 1> | <1 0 1> | 263.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 103.8 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 327.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 148.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 148.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3(CuO3)2 (mvc-11334) | 0.6197 | 0.136 | 3 |
Gd4Au2O9 (mp-623092) | 0.6493 | 0.000 | 3 |
La4Au2O9 (mp-9160) | 0.6631 | 0.000 | 3 |
Sm4Au2O9 (mp-16160) | 0.6444 | 0.000 | 3 |
Nd4Au2O9 (mp-3374) | 0.6416 | 0.000 | 3 |
KSmPdO3 (mp-557232) | 0.0893 | 0.024 | 4 |
KNdPdO3 (mp-558831) | 0.1460 | 0.016 | 4 |
KEuPdO3 (mp-555949) | 0.0948 | 0.873 | 4 |
KLaPdO3 (mp-556475) | 0.2378 | 0.009 | 4 |
KPrPdO3 (mp-560569) | 0.1867 | 0.008 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Gd Pd O |
Final Energy/Atom-7.8276 eV |
Corrected Energy-98.0530 eV
Uncorrected energy = -93.9310 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Corrected energy = -98.0530 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)