Final Magnetic Moment1.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.976 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.909 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 217.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 284.0 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 255.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 210.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 105.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 137.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 144.8 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 217.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 210.3 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 171.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 217.2 |
C (mp-66) | <1 0 0> | <0 1 1> | 256.9 |
C (mp-66) | <1 1 0> | <0 1 1> | 256.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 228.7 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 144.8 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 1> | 171.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 183.0 |
Mg (mp-153) | <1 0 1> | <0 1 1> | 171.3 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 72.4 |
PbS (mp-21276) | <1 1 0> | <0 1 1> | 256.9 |
GaP (mp-2490) | <1 1 0> | <1 0 1> | 210.3 |
GaP (mp-2490) | <1 1 1> | <1 0 1> | 105.1 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 72.4 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 228.7 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 144.8 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 1> | 171.3 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 183.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 183.0 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 217.2 |
PbSe (mp-2201) | <1 1 1> | <1 0 1> | 210.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 144.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 289.6 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 1> | 256.9 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 320.2 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 1> | 210.3 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 183.0 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 137.2 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 320.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 320.2 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 91.5 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 189.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 72.4 |
Si (mp-149) | <1 1 0> | <1 0 1> | 210.3 |
Si (mp-149) | <1 1 1> | <1 0 1> | 105.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 137.2 |
Au (mp-81) | <1 1 0> | <0 1 0> | 72.4 |
Au (mp-81) | <1 1 1> | <1 0 1> | 210.3 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 217.2 |
CdSe (mp-2691) | <1 1 1> | <1 0 1> | 210.3 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 183.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2ReO5 (mp-505390) | 0.2844 | 0.000 | 3 |
Rb2CrF5 (mp-561344) | 0.1577 | 0.099 | 3 |
K2FeF5 (mp-565539) | 0.2570 | 0.000 | 3 |
Rb2CrF5 (mp-622542) | 0.1533 | 0.099 | 3 |
Rb2FeF5 (mp-616339) | 0.0379 | 0.000 | 3 |
Ba4B2N4O (mp-553990) | 0.6994 | 0.011 | 4 |
ReSbOF10 (mp-554432) | 0.6313 | 0.000 | 4 |
Cs4Ru2Cl10O (mp-679984) | 0.6977 | 0.000 | 4 |
CdP2Xe5F22 (mp-556171) | 0.7484 | 0.000 | 4 |
K2TiOF4 (mp-556623) | 0.5933 | 0.000 | 4 |
Te6As4C3(NF8)3 (mp-555419) | 0.7059 | 0.193 | 5 |
K2RuNCl5O (mp-541361) | 0.7335 | 0.000 | 5 |
KWNClF5 (mp-566462) | 0.5799 | 0.106 | 5 |
K2RuNCl5O (mp-560966) | 0.7167 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Rb_sv Fe_pv F |
Final Energy/Atom-4.8273 eV |
Corrected Energy-172.7383 eV
Uncorrected energy = -154.4743 eV
Composition-based energy adjustment (-0.462 eV/atom x 20.0 atoms) = -9.2400 eV
Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV
Corrected energy = -172.7383 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)