Final Magnetic Moment0.996 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.429 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa2V3O7 |
Band Gap2.509 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP31c [159] |
HallP 3 2c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 0 1> | 106.8 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 151.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 107.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 106.8 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 215.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 106.8 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 151.6 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 107.6 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 215.2 |
Mg (mp-153) | <1 1 1> | <1 0 1> | 151.6 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 107.6 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 215.2 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 106.8 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 107.6 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 215.2 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 215.2 |
TiO2 (mp-390) | <1 0 0> | <1 1 0> | 186.4 |
CsI (mp-614603) | <1 1 1> | <0 0 1> | 106.8 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 106.8 |
SrTiO3 (mp-4651) | <1 1 1> | <1 0 0> | 215.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YWN3 (mp-989645) | 0.6173 | 0.015 | 3 |
Li2V3O7 (mp-773375) | 0.6167 | 0.067 | 3 |
LaWN3 (mp-989646) | 0.6039 | 0.016 | 3 |
Na2V3O7 (mp-567133) | 0.1616 | 0.000 | 3 |
LaMoN3 (mp-989534) | 0.5816 | 0.023 | 3 |
LiVO2F (mp-764841) | 0.7431 | 0.049 | 4 |
TiZnBiO5 (mvc-8876) | 0.7347 | 0.081 | 4 |
CaTiBiO5 (mvc-8917) | 0.6565 | 0.059 | 4 |
Ba2Mg2Tl2W3O10 (mvc-3066) | 0.6641 | 0.576 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv V_pv O |
Final Energy/Atom-6.9739 eV |
Corrected Energy-561.8957 eV
-561.8957 eV = -502.1235 eV (uncorrected energy) - 30.2760 eV (MP Advanced Correction) - 29.4962 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)