Final Magnetic Moment0.020 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.111 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSnO2 |
Band Gap0.847 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 279.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 195.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 195.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 279.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 93.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 56.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 97.9 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 232.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 249.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 56.0 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 243.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 293.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 97.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 93.8 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 232.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 195.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 195.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 93.8 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 195.9 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 195.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 251.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 307.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 251.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 251.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 223.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 140.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 93.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 154.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 93.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 97.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 93.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 307.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 279.9 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 246.9 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 232.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 335.9 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 293.6 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 246.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 246.9 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 187.5 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 195.9 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 246.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 93.8 |
Al (mp-134) | <1 1 1> | <1 1 1> | 249.5 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 97.9 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 293.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 249.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 195.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 309.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 223.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2O3F (mp-780038) | 0.2117 | 0.081 | 3 |
BaSrI4 (mp-752514) | 0.2272 | 0.027 | 3 |
Cr(SbO3)2 (mp-769853) | 0.2020 | 0.063 | 3 |
Ni6OF11 (mp-776653) | 0.2288 | 0.038 | 3 |
Cu(SbO3)2 (mp-554658) | 0.2000 | 0.004 | 3 |
LiFe3(OF3)2 (mp-779990) | 0.2429 | 0.005 | 4 |
LiV3(OF3)2 (mp-868491) | 0.2224 | 0.000 | 4 |
LiCo3(OF3)2 (mp-850982) | 0.2165 | 0.022 | 4 |
AlSb(WO4)2 (mvc-665) | 0.2274 | 0.181 | 4 |
AlRe(WO4)2 (mvc-735) | 0.2573 | 0.247 | 4 |
ZrO2 (mp-775980) | 0.1637 | 0.051 | 2 |
BiO2 (mvc-6615) | 0.2062 | 0.021 | 2 |
HfO2 (mp-776097) | 0.1683 | 0.028 | 2 |
CeSe2 (mp-1080630) | 0.2041 | 0.129 | 2 |
SnO2 (mp-550172) | 0.2065 | 0.002 | 2 |
Explore more synthesis descriptions for materials of composition SnO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sn_d O |
Final Energy/Atom-6.2726 eV |
Corrected Energy-242.6690 eV
-242.6690 eV = -225.8140 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)