Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.268 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.574 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 0 0> | <0 0 1> | 216.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 216.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 108.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 108.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 108.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 216.0 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 216.0 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <0 0 1> | 108.0 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 108.0 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 216.0 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 216.0 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 216.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 108.0 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 108.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-557362) | 0.3879 | 0.010 | 3 |
AlPO4 (mp-558056) | 0.3769 | 0.011 | 3 |
Be(PO3)2 (mp-560521) | 0.3943 | 0.003 | 3 |
AlPO4 (mp-667363) | 0.4319 | 0.014 | 3 |
AlPO4 (mp-1019510) | 0.3786 | 0.010 | 3 |
RbAlSiO4 (mp-6434) | 0.7294 | 0.000 | 4 |
CsAlSiO4 (mp-561457) | 0.7133 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.6382 | 0.000 | 4 |
SiO2 (mp-600031) | 0.1454 | 0.011 | 2 |
SiO2 (mp-639506) | 0.1189 | 0.013 | 2 |
SiO2 (mp-557881) | 0.1542 | 0.013 | 2 |
SiO2 (mp-560336) | 0.1475 | 0.013 | 2 |
SiO2 (mp-600083) | 0.1445 | 0.015 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9064 eV |
Corrected Energy-803.9604 eV
-803.9604 eV = -759.0138 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)