Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.269 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.614 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP42/mbc [135] |
Hall-P 4c 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 294.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 251.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 237.5 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 118.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 251.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 196.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 196.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 251.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 167.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 294.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 294.3 |
BN (mp-984) | <1 0 1> | <1 0 1> | 258.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 294.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 294.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 294.3 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 251.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 129.1 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 84.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 251.9 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 251.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 196.2 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 251.9 |
C (mp-48) | <0 0 1> | <1 0 0> | 84.0 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 294.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 251.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 167.9 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 167.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 294.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 294.3 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 196.2 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 294.3 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 251.9 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 251.9 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 251.9 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 251.9 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 196.2 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 167.9 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 294.3 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 251.9 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 167.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 98.1 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 84.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 196.2 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 0> | 118.8 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 237.5 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 251.9 |
Au (mp-81) | <1 1 0> | <1 0 0> | 251.9 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 196.2 |
WS2 (mp-224) | <1 1 0> | <1 1 0> | 237.5 |
ZrO2 (mp-2858) | <1 1 0> | <1 1 0> | 118.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BePO4 (mp-760410) | 0.2639 | 0.063 | 3 |
AlPO4 (mp-707977) | 0.3215 | 0.010 | 3 |
AlPO4 (mp-541338) | 0.3228 | 0.012 | 3 |
AlPO4 (mp-555941) | 0.3591 | 0.011 | 3 |
AlPO4 (mp-559145) | 0.3443 | 0.013 | 3 |
CsBeAsO4 (mp-9113) | 0.7296 | 0.000 | 4 |
Cs2MgSi5O12 (mp-1019610) | 0.7055 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.7005 | 0.000 | 4 |
SiO2 (mp-985590) | 0.1249 | 0.004 | 2 |
SiO2 (mp-18280) | 0.1304 | 0.008 | 2 |
BeF2 (mp-559400) | 0.1319 | 0.002 | 2 |
CeSe2 (mp-1080363) | 0.0493 | 0.524 | 2 |
CeSe2 (mp-1080860) | 0.1351 | 0.525 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9068 eV |
Corrected Energy-402.0020 eV
-402.0020 eV = -379.5287 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)