Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.127 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCe(BO2)3 |
Band Gap0.199 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPca21 [29] |
HallP 2c 2ac |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 214.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 214.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 175.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 311.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 175.4 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 116.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 160.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 194.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 253.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 253.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 155.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 311.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 155.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 116.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 311.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 194.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 251.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 58.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 136.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 311.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 331.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 214.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 232.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 175.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 175.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 331.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 97.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 233.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 97.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 136.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 116.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 214.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 311.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 214.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 370.2 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 175.4 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 331.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 116.9 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 160.8 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 77.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 175.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 214.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 370.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 331.3 |
C (mp-66) | <1 1 0> | <0 1 0> | 160.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 116.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 292.3 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 241.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 214.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 311.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce2B8O15 (mp-1019592) | 0.3611 | 0.027 | 3 |
Y(BO2)3 (mp-768887) | 0.3076 | 0.029 | 3 |
Bi(BO2)3 (mp-554718) | 0.2366 | 0.016 | 3 |
La2B8O15 (mp-1019892) | 0.3735 | 0.023 | 3 |
Ce(BO2)3 (mp-558621) | 0.4459 | 0.000 | 3 |
Ba2Li(BO2)5 (mp-6075) | 0.5233 | 0.000 | 4 |
B5H2Pb2O11 (mp-707942) | 0.5143 | 0.053 | 4 |
CaBeB2O5 (mp-554315) | 0.5734 | 0.004 | 4 |
BaBi2(B2O5)2 (mp-560550) | 0.5418 | 0.000 | 4 |
KSrB5O9 (mp-556250) | 0.6140 | 0.000 | 4 |
Ca2SiB5H5O14 (mp-850516) | 0.6638 | 0.002 | 5 |
KLiZnP2O7 (mp-554164) | 0.7216 | 0.000 | 5 |
Sr2LiBeB3O8 (mp-1020647) | 0.7118 | 0.000 | 5 |
GaGe5H6C4NO12 (mp-684743) | 0.6091 | 0.331 | 6 |
NaLiSiB3HO8 (mp-558267) | 0.5874 | 0.000 | 6 |
ZnBP2H4NO8 (mp-24657) | 0.7256 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce B O |
Final Energy/Atom-8.2715 eV |
Corrected Energy-347.7148 eV
-347.7148 eV = -330.8599 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|