Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.114 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.105 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSO2 + S8O + SOF2 + N2 |
Band Gap1.341 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 291.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 222.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 187.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 222.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 125.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 222.9 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 291.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 297.2 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 118.1 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 297.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 297.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 312.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 187.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 297.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 187.3 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 187.3 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 1> | 291.1 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 291.1 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 125.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 222.9 |
C (mp-66) | <1 1 0> | <0 1 0> | 312.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 222.9 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 312.1 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 74.3 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 291.1 |
PbS (mp-21276) | <1 0 0> | <0 1 1> | 291.1 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 312.1 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 125.4 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 222.9 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 312.1 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 312.1 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 222.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 249.7 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 249.7 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 297.2 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 0> | 312.1 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 0> | 312.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 1> | 291.1 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 0> | 187.3 |
Ga2O3 (mp-886) | <1 1 -1> | <0 1 0> | 249.7 |
Ga2O3 (mp-886) | <1 1 1> | <0 1 0> | 249.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 297.2 |
Au (mp-81) | <1 1 0> | <0 1 0> | 312.1 |
Au (mp-81) | <1 1 1> | <1 0 -1> | 118.1 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 312.1 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 222.9 |
WS2 (mp-224) | <1 0 1> | <0 1 0> | 187.3 |
C (mp-48) | <0 0 1> | <0 1 1> | 291.1 |
C (mp-48) | <1 0 0> | <0 1 0> | 249.7 |
C (mp-48) | <1 0 1> | <0 1 0> | 312.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
S3N2O5 (mp-29224) | 0.5129 | 0.187 | 3 |
H2SO4 (mp-625445) | 0.5507 | 0.030 | 3 |
PNF2 (mp-560275) | 0.5270 | 0.015 | 3 |
C2S7Cl6 (mp-29477) | 0.5352 | 0.092 | 3 |
S2I2O11 (mp-29492) | 0.4111 | 0.005 | 3 |
H2CSO4 (mp-995221) | 0.4924 | 0.305 | 4 |
PNClF (mp-554472) | 0.5873 | 0.008 | 4 |
S5N2ClO6 (mp-555567) | 0.3557 | 0.110 | 4 |
S4N3O2F (mp-556512) | 0.5566 | 0.186 | 4 |
FeS3(NCl2)2 (mp-556297) | 0.4989 | 0.062 | 4 |
Cl2O7 (mp-31050) | 0.6322 | 0.000 | 2 |
CrO3 (mp-776563) | 0.6190 | 0.101 | 2 |
P2O5 (mp-562613) | 0.6454 | 0.010 | 2 |
SeO3 (mp-27519) | 0.6663 | 0.018 | 2 |
SO3 (mp-2414) | 0.5711 | 0.000 | 2 |
P3SN4Cl5O (mp-624218) | 0.6295 | 0.085 | 5 |
FeTeS2N2Cl5 (mp-638705) | 0.5594 | 0.216 | 5 |
CsS2N(O2F)2 (mp-541750) | 0.6514 | 0.073 | 5 |
AlSeS2N2Cl5 (mp-556831) | 0.6476 | 0.075 | 5 |
CS4N2(OF)3 (mp-555309) | 0.4163 | 0.203 | 5 |
NaH2CSO4F3 (mp-601228) | 0.6140 | 0.722 | 6 |
CSe2S2N2(OF)3 (mp-555329) | 0.4323 | 0.222 | 6 |
PS2N3Cl2(OF)2 (mp-558888) | 0.5736 | 0.278 | 6 |
MnGe4H24C8(S5N)2 (mp-698410) | 0.7481 | 0.057 | 6 |
VP2C4N3(ClF6)2 (mp-693133) | 0.7045 | 0.479 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: S N O F |
Final Energy/Atom-5.5095 eV |
Corrected Energy-238.5199 eV
Uncorrected energy = -220.3799 eV
Composition-based energy adjustment (-0.503 eV/atom x 16.0 atoms) = -8.0480 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-0.462 eV/atom x 4.0 atoms) = -1.8480 eV
Corrected energy = -238.5199 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)