Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.246 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.032 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.588 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIa3 [206] |
Hall-I 2b 2c 3 |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 294.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 147.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 208.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 147.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 208.5 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 294.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 221.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 294.8 |
Al (mp-134) | <1 1 0> | <1 1 0> | 208.5 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 294.8 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 104.2 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 127.7 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 104.2 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 147.4 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 104.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 147.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 294.8 |
Si (mp-149) | <1 0 0> | <1 0 0> | 147.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 221.1 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 104.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 73.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 104.2 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 294.8 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 221.1 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 147.4 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 294.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 147.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 221.1 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 294.8 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 208.5 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 208.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 73.7 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 127.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 73.7 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 104.2 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 127.7 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 294.8 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 221.1 |
C (mp-66) | <1 1 1> | <1 0 0> | 221.1 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 147.4 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 73.7 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 73.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 104.2 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 73.7 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 104.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 1> | 255.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 208.5 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 294.8 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 208.5 |
Au (mp-81) | <1 0 0> | <1 0 0> | 294.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5724) | 0.4466 | 0.003 | 3 |
AlPO4 (mp-557362) | 0.4686 | 0.010 | 3 |
AlPO4 (mp-558056) | 0.4276 | 0.011 | 3 |
Be(PO3)2 (mp-560521) | 0.4393 | 0.003 | 3 |
AlPO4 (mp-1019510) | 0.4339 | 0.010 | 3 |
RbAlSiO4 (mp-6434) | 0.6689 | 0.000 | 4 |
CsAlSiO4 (mp-561457) | 0.5719 | 0.000 | 4 |
CsFeSiO4 (mp-644325) | 0.6592 | 0.000 | 4 |
KBePO4 (mp-7324) | 0.7116 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.5943 | 0.000 | 4 |
SiO2 (mp-562490) | 0.2398 | 0.010 | 2 |
CeSe2 (mp-1080261) | 0.2209 | 0.515 | 2 |
CeSe2 (mp-1080273) | 0.2749 | 0.518 | 2 |
CeSe2 (mp-1080326) | 0.2140 | 0.516 | 2 |
SiO2 (mp-557465) | 0.2837 | 0.019 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.8839 eV |
Corrected Energy-200.4512 eV
-200.4512 eV = -189.2146 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)