Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.237 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.041 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.738 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3m [229] |
Hall-I 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5440) | 0.5309 | 0.012 | 3 |
CoPO4 (mp-540391) | 0.5003 | 0.196 | 3 |
AlPO4 (mp-683883) | 0.5416 | 0.018 | 3 |
AlPO4 (mp-560815) | 0.4898 | 0.030 | 3 |
CoPO4 (mp-694829) | 0.4932 | 0.196 | 3 |
RbAlSiO4 (mp-6434) | 0.6504 | 0.000 | 4 |
CsSi3HO7 (mp-758180) | 0.6354 | 0.002 | 4 |
CsAlSiO4 (mp-561457) | 0.6565 | 0.000 | 4 |
CsFeSiO4 (mp-644325) | 0.6611 | 0.000 | 4 |
KBePO4 (mp-7324) | 0.6485 | 0.000 | 4 |
SiO2 (mp-553993) | 0.0941 | 0.039 | 2 |
SiO2 (mp-557930) | 0.3266 | 0.032 | 2 |
SiO2 (mp-559740) | 0.3034 | 0.042 | 2 |
CeSe2 (mp-1087242) | 0.1210 | 0.518 | 2 |
CeSe2 (mp-1094151) | 0.2945 | 0.515 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.8756 eV |
Corrected Energy-1201.5093 eV
-1201.5093 eV = -1134.0895 eV (uncorrected energy) - 67.4198 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)