Final Magnetic Moment0.024 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.778 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn3(AsO4)2 + ZnO |
Band Gap1.614 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <0 0 1> | <0 0 1> | 246.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 246.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 246.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 246.8 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 246.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 246.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 171.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 164.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 171.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 246.8 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 152.1 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 164.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 246.8 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 152.1 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 246.8 |
InP (mp-20351) | <1 1 0> | <1 0 -1> | 152.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 246.8 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 164.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 246.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 246.8 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 164.5 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 246.8 |
Au (mp-81) | <1 0 0> | <0 0 1> | 246.8 |
Au (mp-81) | <1 1 0> | <0 0 1> | 246.8 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 246.8 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 171.0 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 164.5 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 164.5 |
GaTe (mp-542812) | <0 0 1> | <1 0 -1> | 152.1 |
GaTe (mp-542812) | <1 0 -1> | <1 0 -1> | 152.1 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 246.8 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 164.5 |
LiAlO2 (mp-3427) | <1 0 1> | <1 0 0> | 171.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr5(Si2O7)2 (mp-767345) | 0.6748 | 0.100 | 3 |
LiFe2F5 (mp-778405) | 0.6504 | 0.287 | 3 |
Mg(SbO2)2 (mvc-9831) | 0.6423 | 0.218 | 3 |
V2Zn4O9 (mp-504923) | 0.3671 | 0.019 | 3 |
Cr4(PO4)3 (mp-540460) | 0.6798 | 0.324 | 3 |
Li3V3(PO4)4 (mp-763450) | 0.6090 | 0.150 | 4 |
LiNiP2O7 (mp-765968) | 0.5855 | 0.101 | 4 |
Cr4Si2Cl2O7 (mp-567043) | 0.6317 | 0.000 | 4 |
Li3Fe3(PO4)4 (mp-31797) | 0.6372 | 0.049 | 4 |
CaCo2(CuO4)2 (mvc-10489) | 0.5752 | 0.262 | 4 |
K2Mn2Zn4Si4O15 (mp-567173) | 0.7107 | 0.004 | 5 |
Mg5Al4Fe(SiO4)6 (mp-743769) | 0.7160 | 0.280 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn As O |
Final Energy/Atom-5.2821 eV |
Corrected Energy-684.4122 eV
-684.4122 eV = -633.8474 eV (uncorrected energy) - 50.5649 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)