Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.611 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.138 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH4C + H2O + CS14 + NaBr + C |
Band Gap4.288 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 333.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 333.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 333.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 333.1 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 170.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 133.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 266.5 |
Al (mp-134) | <1 1 1> | <1 0 0> | 170.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 199.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 333.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 133.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 333.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 333.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 170.0 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 333.1 |
C (mp-66) | <1 1 0> | <0 0 1> | 333.1 |
Ag (mp-124) | <1 1 1> | <1 0 -1> | 178.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 199.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 66.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 170.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 199.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 333.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 186.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 266.5 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 186.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 266.5 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 133.3 |
C (mp-66) | <1 1 1> | <1 0 -1> | 178.3 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 333.1 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 333.1 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 333.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 199.9 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 170.0 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 133.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 266.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 170.0 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 333.1 |
SiC (mp-11714) | <1 0 0> | <1 0 1> | 186.7 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 266.5 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 266.5 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 199.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 333.1 |
Si (mp-149) | <1 1 0> | <0 0 1> | 333.1 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 186.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 266.5 |
Au (mp-81) | <1 1 1> | <1 0 -1> | 178.3 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 333.1 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 199.9 |
ZnO (mp-2133) | <1 0 1> | <0 1 1> | 257.2 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 199.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
P(H3C)3 (mp-762352) | 0.5419 | 0.049 | 3 |
SiH3I (mp-28538) | 0.5906 | 0.000 | 3 |
AsCF3 (mp-27274) | 0.5972 | 0.494 | 3 |
PCF3 (mp-556383) | 0.4948 | 0.600 | 3 |
Si3PH9 (mp-28842) | 0.5567 | 0.000 | 3 |
H6CIN (mp-997570) | 0.6653 | 0.058 | 4 |
P2H9(CBr)3 (mp-779221) | 0.5695 | 0.000 | 4 |
H9PbC3I (mp-760193) | 0.5514 | 0.206 | 4 |
BPH9C2 (mp-758984) | 0.5621 | 0.072 | 4 |
CIClF4 (mp-556844) | 0.5161 | 0.205 | 4 |
HgH3CSO3 (mp-738615) | 0.6955 | 0.229 | 5 |
SbH12C4NF4 (mp-600218) | 0.6838 | 0.168 | 5 |
InSi2As(H3C)8 (mp-568872) | 0.6649 | 0.073 | 5 |
H3CSClO (mp-644221) | 0.5805 | 0.245 | 5 |
ZnSi4As2(H3C)12 (mp-570146) | 0.6012 | 0.044 | 5 |
H3CSN(ClO)2 (mp-558736) | 0.6275 | 0.455 | 6 |
CdSi3PH27C9Br2 (mp-604998) | 0.7003 | 0.018 | 6 |
AlSiH9C3Cl2O (mp-24308) | 0.6893 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv H C S Br O |
Final Energy/Atom-4.8894 eV |
Corrected Energy-441.1929 eV
-441.1929 eV = -430.2669 eV (uncorrected energy) - 10.9260 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)