Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.960 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.989 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR32 [155] |
HallR 3 2" |
Point Group32 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 348.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 261.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 174.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 369.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 304.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 326.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 152.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 282.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 348.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 282.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 217.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 304.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 108.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 282.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 195.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 261.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 348.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 348.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 87.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 195.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 348.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 348.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 87.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 261.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 261.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 282.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 282.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 261.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 282.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 348.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 87.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 65.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 87.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 21.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 152.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 239.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 282.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 195.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 348.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 348.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 87.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 282.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 132.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 304.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 43.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.35260 | -0.35260 | 0.00000 | 0.27424 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.27424 | -0.35260 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.56908 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
-0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.14 | -0.00 | 0.00 |
-0.00 | 3.14 | 0.00 |
0.00 | 0.00 | 2.98 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.71 | -0.00 | 0.00 |
-0.00 | 9.71 | -0.00 |
0.00 | -0.00 | 7.92 |
Polycrystalline dielectric constant
εpoly∞
3.09
|
Polycrystalline dielectric constant
εpoly
9.12
|
Refractive Index n1.76 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Tl_d S O |
Final Energy/Atom-5.6473 eV |
Corrected Energy-74.2700 eV
Uncorrected energy = -67.7680 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Corrected energy = -74.2700 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)