material

Zn2SiO4

ID:

mp-556163

DOI:

10.17188/1269201


Tags: Dizinc silicate - II Willemite HP Dizinc silicate - t

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.430 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.026 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.49 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Zn2SiO4
Band Gap
2.682 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I42d [122]
Hall
I 4 2bw
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 9147 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
AlN (mp-661) <1 0 1> <1 1 1> 248.5
LaAlO3 (mp-2920) <0 0 1> <1 0 1> 205.6
AlN (mp-661) <1 0 0> <1 1 1> 248.5
AlN (mp-661) <1 1 0> <1 1 0> 328.8
GaAs (mp-2534) <1 0 0> <0 0 1> 251.8
GaN (mp-804) <1 0 1> <1 0 0> 232.5
CeO2 (mp-20194) <1 0 0> <0 0 1> 251.8
BaF2 (mp-1029) <1 0 0> <0 0 1> 201.4
GaN (mp-804) <0 0 1> <1 0 0> 186.0
GaN (mp-804) <1 1 0> <1 0 0> 232.5
SiO2 (mp-6930) <1 0 0> <1 1 0> 197.3
KCl (mp-23193) <1 1 0> <1 0 0> 232.5
DyScO3 (mp-31120) <0 1 1> <1 1 1> 165.6
DyScO3 (mp-31120) <1 1 0> <0 0 1> 251.8
DyScO3 (mp-31120) <1 1 1> <1 0 0> 139.5
SiO2 (mp-6930) <1 1 0> <1 1 0> 328.8
KCl (mp-23193) <1 0 0> <0 0 1> 201.4
DyScO3 (mp-31120) <1 0 1> <1 0 1> 274.1
InAs (mp-20305) <1 0 0> <0 0 1> 201.4
ZnSe (mp-1190) <1 0 0> <0 0 1> 251.8
ZnSe (mp-1190) <1 1 0> <1 0 1> 137.1
KTaO3 (mp-3614) <1 0 0> <1 0 0> 325.5
KTaO3 (mp-3614) <1 1 0> <1 0 1> 68.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 251.8
CdS (mp-672) <0 0 1> <0 0 1> 151.1
CdS (mp-672) <1 1 1> <1 0 1> 205.6
LiF (mp-1138) <1 0 0> <1 0 0> 325.5
Te2W (mp-22693) <0 0 1> <1 0 0> 279.0
YVO4 (mp-19133) <1 0 0> <1 0 0> 46.5
YVO4 (mp-19133) <1 0 1> <1 0 1> 68.5
YVO4 (mp-19133) <1 1 0> <1 1 0> 65.8
YVO4 (mp-19133) <1 1 1> <0 0 1> 251.8
Te2W (mp-22693) <0 1 0> <1 0 0> 325.5
Te2W (mp-22693) <0 1 1> <1 0 0> 232.5
YVO4 (mp-19133) <0 0 1> <0 0 1> 50.4
TePb (mp-19717) <1 0 0> <1 1 0> 131.5
Te2Mo (mp-602) <1 0 1> <1 1 0> 328.8
Ag (mp-124) <1 0 0> <1 1 0> 263.0
Ag (mp-124) <1 1 0> <1 0 1> 274.1
Ag (mp-124) <1 1 1> <0 0 1> 151.1
TePb (mp-19717) <1 1 0> <1 0 0> 186.0
Te2Mo (mp-602) <1 0 0> <1 0 0> 325.5
GaSe (mp-1943) <0 0 1> <1 0 0> 325.5
GaSe (mp-1943) <1 1 1> <1 0 0> 232.5
BN (mp-984) <1 0 0> <0 0 1> 151.1
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 325.5
GaSe (mp-1943) <1 1 0> <1 0 0> 232.5
BN (mp-984) <0 0 1> <1 0 0> 325.5
BN (mp-984) <1 0 1> <1 1 0> 263.0
MoS2 (mp-1434) <1 0 0> <1 0 0> 139.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.43894 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 -0.06316 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 -0.06316
Piezoelectric Modulus ‖eijmax
0.43894 C/m2
Crystallographic Direction vmax
1.00000
0.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.38 0.00 0.00
0.00 3.45 0.00
0.00 0.00 3.45
Dielectric Tensor εij (total)
9.40 0.00 0.00
0.00 9.31 0.00
0.00 0.00 9.31
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.43
Polycrystalline dielectric constant εpoly
(total)
9.34
Refractive Index n
1.85
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zn2SiO4 (mp-3789) 0.3755 0.000 3
Na2CrO4 (mp-764193) 0.4343 0.018 3
Li2CrO4 (mp-24920) 0.3826 0.000 3
Li2BeF4 (mp-4622) 0.3602 0.000 3
Li2SeO4 (mp-4855) 0.3827 0.000 3
LiCoPO4 (mp-31541) 0.3255 0.002 4
LiFePO4 (mp-585400) 0.3060 0.212 4
LiNiPO4 (mp-32350) 0.3218 0.077 4
LiCoPO4 (mp-585404) 0.3263 0.002 4
LiNiPO4 (mp-540255) 0.3323 0.031 4
Sm3S4 (mp-673636) 0.5963 0.417 2
BN (mp-1077506) 0.5934 0.302 2
SiC2 (mp-1019097) 0.3607 0.562 2
CN2 (mp-1009818) 0.5722 0.714 2
Ge3N4 (mp-571281) 0.5677 0.063 2
Li4Ga3Si3IO12 (mp-557112) 0.4731 0.000 5
Li4Ga3Si3ClO12 (mp-554203) 0.4866 0.000 5
Li4Ga3Si3BrO12 (mp-556649) 0.4770 0.000 5
Mn4Be3Ge3SeO12 (mp-25766) 0.5691 0.000 5
Mn4Be3Ge3SO12 (mp-25772) 0.5710 0.000 5
Na2Li2Al3Si3ClO12 (mp-43030) 0.7098 0.003 6
C (mp-568410) 0.5941 0.507 1
C (mp-1008374) 0.5584 0.437 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

The preparation of Si-NPA has been described in detail elsewhere [17]. The growing of Zn2SiO4 on Si-NPA was conducted in a horizontal tube furnace. The mixture of 0.4g ZnO and 0.1g graphite, which w [...]
The Zn2SiO4 ceramics with the addition of BaO and B2O3 are fabricated by traditional solid-state preparation process at a sintering temperature of 900C. The introduction of BaO and B2O3 to the binar [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition Zn2SiO4.

Text computed by synthesisproject.org.

Calculation Summary

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zn Si O
Final Energy/Atom
-5.9912 eV
Corrected Energy
-89.3723 eV
Uncorrected energy = -83.8763 eV Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV Corrected energy = -89.3723 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 9147
  • 167188
Submitted by
User remarks:
  • Dizinc silicate - II
  • Willemite HP

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)