Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.384 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.097 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaSc3(BO3)4 |
Band Gap3.885 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR32 [155] |
HallR 3 2" |
Point Group32 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 160.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 164.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 245.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 240.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 245.9 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 80.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 245.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 160.4 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 160.4 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 164.0 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 160.4 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 160.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 240.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 80.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 142.0 |
Au (mp-81) | <1 0 0> | <1 0 0> | 245.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 240.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 245.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 245.9 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 240.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 245.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 240.6 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 1> | 229.4 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 142.0 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 164.0 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 245.9 |
PbS (mp-21276) | <1 0 0> | <1 1 0> | 142.0 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 240.6 |
InP (mp-20351) | <1 0 0> | <1 1 0> | 142.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 240.6 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 245.9 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 80.2 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 0> | 142.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 240.6 |
Au (mp-81) | <1 1 0> | <1 0 0> | 245.9 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 245.9 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 240.6 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 160.4 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 245.9 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 240.6 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 80.2 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 0> | 245.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BiBO3 (mp-31250) | 0.4335 | 0.000 | 3 |
BaCO3 (mp-675324) | 0.4390 | 0.076 | 3 |
KNO3 (mp-676851) | 0.4409 | 0.011 | 3 |
AgNO3 (mp-552185) | 0.4789 | 0.000 | 3 |
MnCO3 (mp-1078473) | 0.3006 | 0.030 | 3 |
LiV(CO3)2 (mp-765385) | 0.4563 | 0.065 | 4 |
LiV(CO3)2 (mp-763059) | 0.2054 | 0.096 | 4 |
CaMg3(CO3)4 (mp-6524) | 0.4777 | 0.004 | 4 |
CeSc3(BO3)4 (mp-16097) | 0.5053 | 0.000 | 4 |
BaCa(CO3)2 (mp-644852) | 0.4795 | 0.014 | 4 |
LiVCO3F2 (mp-767837) | 0.6734 | 0.070 | 5 |
NaSbCO2F3 (mp-554239) | 0.7267 | 0.031 | 5 |
NaSbCO2F3 (mp-554716) | 0.7214 | 0.031 | 5 |
NaCdH3(CO2)3 (mp-557366) | 0.7038 | 0.107 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Sc_sv B O |
Final Energy/Atom-8.4639 eV |
Corrected Energy-177.7061 eV
-177.7061 eV = -169.2787 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)