Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-1.128 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZnS |
Band Gap2.064 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 321.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 115.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 347.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 231.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 270.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 205.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 205.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 51.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 270.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 193.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 167.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 205.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 270.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 257.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 373.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 90.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 360.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 231.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 205.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 283.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 321.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 270.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 308.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 205.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 270.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 193.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 167.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 270.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 257.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 115.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 205.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 257.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 334.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 270.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 193.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 90.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 347.3 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 167.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 128.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 308.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 167.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 270.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 270.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 193.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 90.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 51.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 12.9 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 205.8 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 115.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoSi(CuS2)2 (mp-11769) | 0.1062 | 0.074 | 4 |
MnAg2GeTe4 (mp-1025568) | 0.1221 | 0.007 | 4 |
FeSi(CuSe2)2 (mp-1025510) | 0.1081 | 0.055 | 4 |
FeCu2GeS4 (mp-22053) | 0.1130 | 0.041 | 4 |
CoCu2GeS4 (mp-6498) | 0.1099 | 0.061 | 4 |
ZnS (mp-555763) | 0.0107 | 0.003 | 2 |
ZnS (mp-555410) | 0.0218 | 0.002 | 2 |
ZnS (mp-556005) | 0.0220 | 0.001 | 2 |
ZnS (mp-554405) | 0.0092 | 0.003 | 2 |
ZnS (mp-543011) | 0.0155 | 0.012 | 2 |
AlCuS2 (mvc-16090) | 0.1026 | 0.000 | 3 |
BeSiN2 (mp-15704) | 0.1008 | 0.001 | 3 |
InAgTe2 (mp-22386) | 0.1020 | 0.000 | 3 |
GaCuSe2 (mp-4840) | 0.1017 | 0.000 | 3 |
FeCuS2 (mp-640073) | 0.1022 | 0.111 | 3 |
C (mp-611426) | 0.0349 | 0.145 | 1 |
C (mp-569567) | 0.0461 | 0.174 | 1 |
C (mp-616440) | 0.0491 | 0.141 | 1 |
C (mp-569517) | 0.0391 | 0.145 | 1 |
C (mp-611448) | 0.0434 | 0.142 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points10 |
U Values-- |
PseudopotentialsVASP PAW: Zn S |
Final Energy/Atom-3.4960 eV |
Corrected Energy-61.2434 eV
-61.2434 eV = -55.9357 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)