Final Magnetic Moment3.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.210 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa3Bi2RuO9 + BaRuO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 1> | 109.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 125.5 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 168.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 251.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 313.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 313.7 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 168.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 313.7 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 168.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 313.7 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 188.2 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 188.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 313.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 125.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 188.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 251.0 |
BN (mp-984) | <1 0 0> | <0 1 0> | 267.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 267.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 188.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 313.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 313.7 |
Al (mp-134) | <1 1 0> | <0 0 1> | 313.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 168.9 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 188.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 313.7 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 188.2 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 188.2 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 313.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 125.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 62.7 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 178.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 313.7 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 125.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 0> | 155.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 251.0 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 251.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 251.0 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 155.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 251.0 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 155.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 251.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 313.7 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 313.7 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 125.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 218.3 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 313.7 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 62.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 313.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 313.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 125.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr4Nb2O9 (mp-675416) | 0.6014 | 0.084 | 3 |
SrMnO3 (mp-568977) | 0.5582 | 0.000 | 3 |
Ca3GeO (mp-17193) | 0.5902 | 0.000 | 3 |
LaAlO3 (mp-1080060) | 0.5981 | 0.001 | 3 |
KCrF3 (mp-566698) | 0.5872 | 0.000 | 3 |
Ba2PrRuO6 (mp-984806) | 0.4441 | 0.005 | 4 |
Ba2LaIrO6 (mp-15889) | 0.4390 | 0.000 | 4 |
Ba3SrIr2O9 (mp-554266) | 0.3936 | 0.000 | 4 |
Ba2LaRuO6 (mp-554410) | 0.4506 | 0.001 | 4 |
Ba2NdRuO6 (mp-6200) | 0.4497 | 0.000 | 4 |
Ba18Pr9Sn4Sb5O54 (mp-695389) | 0.6457 | 0.040 | 5 |
Sr11LaFe6(MoO6)6 (mp-735565) | 0.6328 | 0.009 | 5 |
Sr2La2MgTi3O12 (mp-694982) | 0.5531 | 0.029 | 5 |
Na3SrTiNb3O12 (mp-677431) | 0.6045 | 0.029 | 5 |
KBaBiTeO6 (mp-1040443) | 0.4822 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Bi Ru_pv O |
Final Energy/Atom-6.6369 eV |
Corrected Energy-211.7493 eV
-211.7493 eV = -199.1081 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)