material

KSb(PS3)2

ID:

mp-556609

DOI:

10.17188/1269447


Tags: Potassium antimony hexathiodiphosphate(IV)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.778 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.62 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.273 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21 [4]
Hall
P 2yb
Point Group
2
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 409751 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <0 0 1> <0 1 1> 0.001 256.6
SiC (mp-7631) <0 0 1> <0 1 1> 0.001 256.6
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.004 213.0
KCl (mp-23193) <1 1 1> <0 0 1> 0.004 213.0
AlN (mp-661) <0 0 1> <0 0 1> 0.005 213.0
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.008 213.0
C (mp-48) <1 1 0> <1 0 0> 0.009 234.1
ZnO (mp-2133) <1 0 0> <1 0 0> 0.010 156.1
Au (mp-81) <1 1 1> <0 0 1> 0.011 213.0
CsI (mp-614603) <1 0 0> <1 0 0> 0.014 312.1
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.016 266.3
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.017 288.9
C (mp-48) <1 0 0> <1 0 0> 0.018 78.0
Ag (mp-124) <1 1 1> <0 0 1> 0.022 213.0
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.024 234.1
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.025 213.0
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.028 205.6
GdScO3 (mp-5690) <1 1 0> <1 0 1> 0.030 192.6
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.033 267.7
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.033 312.1
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.034 106.5
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.034 156.1
TbScO3 (mp-31119) <1 1 0> <1 0 1> 0.035 192.6
GaN (mp-804) <1 0 1> <0 0 1> 0.035 319.5
CsI (mp-614603) <1 1 0> <0 0 1> 0.037 266.3
PbS (mp-21276) <1 0 0> <1 0 1> 0.039 288.9
BaTiO3 (mp-5986) <0 0 1> <1 0 1> 0.039 96.3
TiO2 (mp-390) <0 0 1> <1 0 1> 0.039 288.9
CdS (mp-672) <1 0 0> <1 0 0> 0.039 312.1
MgO (mp-1265) <1 0 0> <1 0 1> 0.039 288.9
C (mp-66) <1 0 0> <1 0 1> 0.041 192.6
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.042 312.1
DyScO3 (mp-31120) <1 1 0> <1 0 1> 0.042 192.6
Si (mp-149) <1 1 0> <0 0 1> 0.043 213.0
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.043 213.0
C (mp-48) <0 0 1> <0 1 0> 0.043 267.7
LiF (mp-1138) <1 0 0> <0 0 1> 0.044 319.5
Fe3O4 (mp-19306) <1 0 0> <1 0 1> 0.044 288.9
LiF (mp-1138) <1 1 1> <1 0 0> 0.046 234.1
BN (mp-984) <1 0 0> <1 0 0> 0.047 78.0
KTaO3 (mp-3614) <1 0 0> <1 0 1> 0.052 96.3
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.053 192.6
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.054 266.3
GaP (mp-2490) <1 1 0> <0 0 1> 0.056 213.0
TbScO3 (mp-31119) <0 1 0> <0 1 0> 0.057 133.8
InSb (mp-20012) <1 0 0> <0 0 1> 0.057 266.3
TeO2 (mp-2125) <1 1 0> <1 0 1> 0.058 96.3
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.060 205.6
CdTe (mp-406) <1 0 0> <0 0 1> 0.061 266.3
SiC (mp-11714) <1 0 0> <1 0 0> 0.063 156.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
19 8 8 0 -3 0
8 15 6 0 0 0
8 6 22 0 -1 0
0 0 0 7 0 -2
-3 0 -1 0 7 0
0 0 0 -2 0 9
Compliance Tensor Sij (10-12Pa-1)
84.2 -38 -20.5 0 35.8 0
-38 93.4 -11.6 0 -20.6 0
-20.5 -11.6 56.1 0 -1.3 0
0 0 0 140.3 0 26.6
35.8 -20.6 -1.3 0 151.9 0
0 0 0 26.6 0 115.4
Shear Modulus GV
7 GPa
Bulk Modulus KV
11 GPa
Shear Modulus GR
6 GPa
Bulk Modulus KR
11 GPa
Shear Modulus GVRH
7 GPa
Bulk Modulus KVRH
11 GPa
Elastic Anisotropy
0.74
Poisson's Ratio
0.25

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.01594 0.00000 -0.09605
-0.05023 -0.31269 -0.32737 0.00000 -0.07140 0.00000
0.00000 0.00000 0.00000 -0.39819 0.00000 -0.05727
Piezoelectric Modulus ‖eijmax
0.46105 C/m2
Crystallographic Direction vmax
0.00000
0.00000
1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.83 0.00 -0.23
0.00 5.13 0.00
-0.23 0.00 5.28
Dielectric Tensor εij (total)
11.96 0.00 -1.34
0.00 10.21 0.00
-1.34 0.00 12.02
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.08
Polycrystalline dielectric constant εpoly
(total)
11.40
Refractive Index n
2.25
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cs2Hg3I8 (mp-540574) 0.5130 0.000 3
Ba3Sb4O (mp-555414) 0.5688 0.000 3
K2PO4 (mp-555840) 0.6112 0.090 3
SnPS3 (mp-13923) 0.6286 0.000 3
KAl2Br7 (mp-30978) 0.6110 0.000 3
KSb(PSe3)2 (mp-7123) 0.1717 0.000 4
NaSb(PS3)2 (mp-561303) 0.4800 0.008 4
KBi(PS3)2 (mp-557437) 0.4522 0.000 4
KBi(PSe3)2 (mp-568802) 0.4962 0.003 4
TlBi(PS3)2 (mp-556592) 0.4420 0.000 4
GaBr2 (mp-650841) 0.7382 0.011 2
Ga3Cl7 (mp-616204) 0.7212 0.010 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: K_sv Sb P S
Final Energy/Atom
-4.5645 eV
Corrected Energy
-97.3269 eV
Uncorrected energy = -91.2909 eV Composition-based energy adjustment (-0.503 eV/atom x 12.0 atoms) = -6.0360 eV Corrected energy = -97.3269 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 409751
Submitted by
User remarks:
  • Potassium antimony hexathiodiphosphate(IV)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)