Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.901 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.268 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 208.1 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 285.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 208.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 118.3 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 158.8 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 190.5 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 138.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 310.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 236.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 138.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 251.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 274.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 221.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 207.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 207.1 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 219.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 118.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 251.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 44.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 221.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 74.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 95.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 103.8 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 274.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 221.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 349.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 219.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 208.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 138.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 276.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 267.6 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 103.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 281.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 133.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 236.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 138.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 147.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 69.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 138.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 295.9 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 285.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 133.1 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 254.0 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 316.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 295.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 118.3 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 69.2 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 254.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 173.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 254.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrSbO4 (mp-771809) | 0.4731 | 0.120 | 3 |
NiTeO4 (mp-774160) | 0.4112 | 0.099 | 3 |
FeCoO4 (mp-771871) | 0.4437 | 0.133 | 3 |
Fe2Co3O10 (mp-778217) | 0.4653 | 0.119 | 3 |
Mn3FeO8 (mp-771261) | 0.4709 | 0.100 | 3 |
LiFe5(OF2)4 (mp-782691) | 0.6113 | 0.081 | 4 |
CaNiWO6 (mvc-14986) | 0.5564 | 0.303 | 4 |
Mn3Cr3(WO8)2 (mp-778921) | 0.5852 | 0.103 | 4 |
LiV(OF)2 (mp-764229) | 0.5457 | 0.031 | 4 |
Mn3V2Cr3O16 (mp-773144) | 0.6304 | 0.084 | 4 |
FeO2 (mp-714904) | 0.3024 | 0.381 | 2 |
VO2 (mp-714944) | 0.3475 | 0.138 | 2 |
VO2 (mp-714960) | 0.3809 | 0.159 | 2 |
FeO2 (mp-1062652) | 0.3944 | 0.254 | 2 |
CoO2 (mp-1077196) | 0.0519 | 0.164 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co O |
Final Energy/Atom-5.4766 eV |
Corrected Energy-19.7085 eV
-19.7085 eV = -16.4299 eV (uncorrected energy) - 1.8740 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)